Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.497 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density11.85 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mcm [193] |
Hall-P 6c 2 |
Point Group6/mmm |
Crystal Systemhexagonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 0 0> | 298.6 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 99.5 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 199.1 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 199.1 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 248.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 64.1 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 298.6 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 248.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 248.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 348.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 199.1 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 248.9 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 320.3 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 320.3 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 149.3 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 258.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 258.6 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 348.4 |
LiF (mp-1138) | <1 0 0> | <1 1 1> | 214.8 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 172.4 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 162.3 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 64.1 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 99.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 192.2 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 243.4 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 258.6 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 256.3 |
Te2Mo (mp-602) | <0 0 1> | <1 0 1> | 243.4 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 320.3 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 192.2 |
TePb (mp-19717) | <1 0 0> | <1 1 1> | 214.8 |
GaSe (mp-1943) | <0 0 1> | <1 1 1> | 214.8 |
GaSe (mp-1943) | <1 0 0> | <1 1 0> | 258.6 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 298.6 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 172.4 |
Ag (mp-124) | <1 1 1> | <1 0 1> | 243.4 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 248.9 |
BN (mp-984) | <0 0 1> | <1 0 0> | 348.4 |
BN (mp-984) | <1 1 0> | <0 0 1> | 64.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 1> | 243.4 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 128.1 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 192.2 |
CdTe (mp-406) | <1 0 0> | <1 1 1> | 214.8 |
Al (mp-134) | <1 0 0> | <1 1 1> | 214.8 |
Al (mp-134) | <1 1 0> | <1 1 0> | 258.6 |
Al (mp-134) | <1 1 1> | <0 0 1> | 192.2 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 99.5 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 149.3 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 256.3 |
MgO (mp-1265) | <1 1 1> | <1 0 1> | 243.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Zr5AlSn3 (mp-510321) | 0.0470 | 0.000 | 3 |
U3NbSb5 (mp-570831) | 0.0694 | 0.079 | 3 |
Zr5ZnSb3 (mp-10870) | 0.0742 | 0.000 | 3 |
HfU3Sb5 (mp-12890) | 0.0558 | 0.066 | 3 |
ScU3Sb5 (mp-13243) | 0.0428 | 0.000 | 3 |
Gd3Ti2MnSi3 (mp-569019) | 0.3147 | 0.407 | 4 |
Zr5Sn4 (mp-543001) | 0.2384 | 0.000 | 2 |
Nb5Ga4 (mp-18032) | 0.2150 | 0.008 | 2 |
Zr5Sb4 (mp-570196) | 0.2617 | 0.020 | 2 |
Hf5Sn4 (mp-510691) | 0.2762 | 0.000 | 2 |
Th5Sn4 (mp-30874) | 0.2086 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Hf_pv Zn Sb |
Final Energy/Atom-7.5450 eV |
Corrected Energy-135.8102 eV
-135.8102 eV = -135.8102 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)