Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.217 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.247 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.38 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToH4C + H2O + C |
Band Gap2.841 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbcn [60] |
Hall-P 2n 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 326.5 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 91.0 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 108.8 |
BaF2 (mp-1029) | <1 0 0> | <1 1 0> | 192.0 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 54.4 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 212.5 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 318.6 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 318.6 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 212.8 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 163.3 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 45.5 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 227.5 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 91.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 45.5 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 54.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 45.5 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 54.4 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 283.8 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 318.6 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 136.5 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 141.9 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 316.3 |
InAs (mp-20305) | <1 0 0> | <1 1 0> | 192.0 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 163.3 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 45.5 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 227.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 163.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 54.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 45.5 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 108.8 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 227.5 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 288.0 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 237.3 |
Te2W (mp-22693) | <0 1 0> | <0 1 1> | 212.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 136.5 |
LiF (mp-1138) | <1 1 1> | <1 1 0> | 288.0 |
YVO4 (mp-19133) | <1 0 1> | <1 1 0> | 288.0 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 182.0 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 136.5 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 318.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 326.5 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 318.6 |
BN (mp-984) | <0 0 1> | <1 1 1> | 212.5 |
BN (mp-984) | <1 0 1> | <0 0 1> | 318.6 |
BN (mp-984) | <1 1 1> | <1 0 0> | 237.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 108.8 |
MoS2 (mp-1434) | <0 0 1> | <0 1 1> | 70.9 |
Al (mp-134) | <1 0 0> | <0 1 0> | 163.3 |
Al (mp-134) | <1 1 0> | <0 0 1> | 45.5 |
Al (mp-134) | <1 1 1> | <0 1 0> | 54.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
KN3O4 (mp-3768) | 0.5975 | 0.181 | 3 |
C2O3F2 (mp-31306) | 0.4538 | 0.165 | 3 |
NClO3 (mp-754712) | 0.6532 | 0.000 | 3 |
AgN3O4 (mp-644729) | 0.5495 | 0.183 | 3 |
HSN (mp-29349) | 0.6513 | 0.176 | 3 |
H2C3(N2Cl)2 (mp-698476) | 0.6412 | 0.017 | 4 |
C2S(NCl)3 (mp-558545) | 0.6798 | 0.100 | 4 |
H6C(N3O2)2 (mp-707543) | 0.5734 | 0.320 | 4 |
H4C(N2O)2 (mp-707535) | 0.5724 | 0.275 | 4 |
CS2(NCl)3 (mp-560879) | 0.7201 | 0.183 | 4 |
C4O3 (mp-1001594) | 0.5335 | 0.236 | 2 |
HN (mp-684592) | 0.6647 | 0.298 | 2 |
CO2 (mp-995224) | 0.5819 | 0.297 | 2 |
CO2 (mp-995198) | 0.5596 | 0.319 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: H C O |
Final Energy/Atom-6.8139 eV |
Corrected Energy-302.6187 eV
-302.6187 eV = -299.8095 eV (uncorrected energy) - 2.8092 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)