Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.175 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.061 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.90 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCs4Si3O8 + CsH3O2 |
Band Gap3.973 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 -1> | 224.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 141.3 |
GaAs (mp-2534) | <1 1 0> | <0 1 -1> | 278.3 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 202.9 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 270.5 |
AlN (mp-661) | <1 1 0> | <1 -1 0> | 292.5 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 141.3 |
CeO2 (mp-20194) | <1 0 0> | <1 0 -1> | 336.0 |
CeO2 (mp-20194) | <1 1 0> | <1 0 -1> | 168.0 |
GaAs (mp-2534) | <1 0 0> | <1 -1 0> | 292.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 353.3 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 152.6 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 254.3 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 212.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 247.3 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 268.6 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 214.9 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 -1> | 224.0 |
SiO2 (mp-6930) | <0 0 1> | <1 -1 0> | 219.4 |
SiO2 (mp-6930) | <1 1 0> | <1 0 -1> | 280.0 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 214.9 |
ZnSe (mp-1190) | <1 1 0> | <0 1 -1> | 278.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 214.9 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 214.9 |
InAs (mp-20305) | <1 1 1> | <1 -1 -1> | 318.3 |
ZnSe (mp-1190) | <1 0 0> | <0 1 -1> | 222.7 |
CdS (mp-672) | <0 0 1> | <1 -1 1> | 248.4 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 176.6 |
CdS (mp-672) | <1 1 1> | <1 1 -1> | 214.5 |
KTaO3 (mp-3614) | <1 0 0> | <1 -1 0> | 146.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 1> | 92.7 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 254.3 |
LiF (mp-1138) | <1 0 0> | <0 1 -1> | 222.7 |
LiF (mp-1138) | <1 1 0> | <0 1 -1> | 167.0 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 176.6 |
Te2W (mp-22693) | <1 0 0> | <1 1 -1> | 286.0 |
YVO4 (mp-19133) | <1 0 0> | <0 1 -1> | 278.3 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 305.2 |
TePb (mp-19717) | <1 1 1> | <1 0 -1> | 224.0 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 282.6 |
Te2Mo (mp-602) | <1 1 0> | <1 0 1> | 286.6 |
YVO4 (mp-19133) | <1 1 0> | <1 0 -1> | 336.0 |
YVO4 (mp-19133) | <1 1 1> | <0 1 0> | 254.3 |
Ag (mp-124) | <1 1 0> | <0 1 -1> | 167.0 |
Ag (mp-124) | <1 1 1> | <1 0 -1> | 336.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 -1> | 222.7 |
Te2Mo (mp-602) | <1 1 1> | <1 1 -1> | 286.0 |
Ag (mp-124) | <1 0 0> | <0 1 -1> | 222.7 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 212.0 |
BN (mp-984) | <0 0 1> | <0 1 0> | 203.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Hg3(AsO4)2 (mp-8975) | 0.6248 | 0.000 | 3 |
Al2Hg3Cl8 (mp-27346) | 0.6702 | 0.000 | 3 |
CrAgO4 (mp-849702) | 0.6193 | 0.423 | 3 |
V2Bi4O11 (mp-690568) | 0.6055 | 0.074 | 3 |
Hg3(PO4)2 (mp-12199) | 0.6553 | 0.000 | 3 |
CaB2(HO)8 (mp-721875) | 0.5497 | 0.037 | 4 |
NaB(HO)4 (mp-707419) | 0.4804 | 0.006 | 4 |
NaGa(H2N)4 (mp-706544) | 0.5521 | 0.006 | 4 |
KP(HO2)2 (mp-604119) | 0.5585 | 0.057 | 4 |
Sb4H2SO10 (mp-698480) | 0.5731 | 0.000 | 4 |
LiCrPH2O5 (mp-781961) | 0.6092 | 0.253 | 5 |
RbH4SNO4 (mp-555770) | 0.6056 | 0.005 | 5 |
K3GeH2NO3 (mp-697540) | 0.6115 | 0.000 | 5 |
KZnH4Br3O2 (mp-720912) | 0.5825 | 0.016 | 5 |
Li2SbSO4F3 (mp-769153) | 0.5900 | 0.069 | 5 |
KLiH4S2(NO3)2 (mp-699460) | 0.7091 | 0.053 | 6 |
SiBHC3NCl2 (mp-698440) | 0.5444 | 0.908 | 6 |
Na2TeHSO5F3 (mp-696485) | 0.7008 | 0.016 | 6 |
FePH5NO4F (mp-705481) | 0.6134 | 0.649 | 6 |
AgH8C4S3(OF)3 (mp-605808) | 0.7060 | 0.263 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cs_sv Si H O |
Final Energy/Atom-5.5834 eV |
Corrected Energy-106.1198 eV
-106.1198 eV = -100.5015 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)