Material Details

Final Magnetic Moment
0.024 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.809 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.56 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 42921 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CdS (mp-672) <0 0 1> <0 0 1> 0.000 107.2
BN (mp-984) <1 1 0> <1 0 0> 0.001 201.4
Ga2O3 (mp-886) <1 0 1> <0 0 1> 0.001 231.0
CsI (mp-614603) <1 1 1> <0 0 1> 0.004 107.2
GaN (mp-804) <0 0 1> <0 0 1> 0.004 107.2
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.006 33.0
Ga2O3 (mp-886) <1 0 -1> <0 0 1> 0.007 115.5
BaF2 (mp-1029) <1 1 1> <1 0 1> 0.008 205.6
Ge (mp-32) <1 1 1> <0 0 1> 0.011 57.7
SrTiO3 (mp-4651) <1 0 1> <0 0 1> 0.016 107.2
SiC (mp-11714) <0 0 1> <0 0 1> 0.018 8.2
GaP (mp-2490) <1 1 1> <0 0 1> 0.020 156.7
SiC (mp-7631) <0 0 1> <0 0 1> 0.023 8.2
TePb (mp-19717) <1 1 1> <0 0 1> 0.025 74.2
Mg (mp-153) <1 0 1> <1 0 1> 0.033 246.7
SiC (mp-8062) <1 1 1> <0 0 1> 0.034 33.0
InAs (mp-20305) <1 1 0> <1 0 0> 0.036 161.1
BN (mp-984) <1 0 1> <0 0 1> 0.036 222.7
Te2Mo (mp-602) <1 0 0> <0 0 1> 0.043 165.0
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.046 173.2
ZnTe (mp-2176) <1 1 0> <1 0 0> 0.048 161.1
GaAs (mp-2534) <1 1 1> <0 0 1> 0.051 57.7
Si (mp-149) <1 1 1> <0 0 1> 0.054 156.7
CaF2 (mp-2741) <1 1 1> <0 0 1> 0.057 156.7
SiC (mp-11714) <1 1 1> <0 0 1> 0.058 272.2
CeO2 (mp-20194) <1 1 1> <0 0 1> 0.061 156.7
TiO2 (mp-390) <1 1 0> <1 1 0> 0.070 209.3
TePb (mp-19717) <1 1 0> <1 0 0> 0.073 120.8
C (mp-66) <1 1 0> <1 0 0> 0.076 161.1
BaTiO3 (mp-5986) <1 0 1> <1 0 1> 0.085 164.5
WSe2 (mp-1821) <1 0 1> <1 0 1> 0.086 205.6
SiC (mp-8062) <1 1 0> <1 0 0> 0.088 80.6
ZnSe (mp-1190) <1 1 1> <0 0 1> 0.090 57.7
ZnO (mp-2133) <1 0 0> <1 1 0> 0.094 69.8
ZrO2 (mp-2858) <1 1 0> <0 0 1> 0.094 198.0
C (mp-66) <1 1 1> <0 0 1> 0.101 156.7
Cu (mp-30) <1 1 1> <0 0 1> 0.102 156.7
SiO2 (mp-6930) <1 0 1> <0 0 1> 0.105 313.5
C (mp-48) <0 0 1> <0 0 1> 0.105 99.0
TiO2 (mp-390) <1 1 1> <0 0 1> 0.118 272.2
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.121 156.7
BN (mp-984) <1 0 0> <0 0 1> 0.127 156.7
LiGaO2 (mp-5854) <1 1 1> <0 0 1> 0.131 165.0
WS2 (mp-224) <0 0 1> <0 0 1> 0.135 107.2
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.136 107.2
ZrO2 (mp-2858) <1 1 -1> <1 0 0> 0.142 322.2
YAlO3 (mp-3792) <1 0 0> <0 0 1> 0.148 198.0
KP(HO2)2 (mp-23959) <0 1 0> <0 0 1> 0.165 231.0
TiO2 (mp-2657) <1 0 0> <0 0 1> 0.167 222.7
MoSe2 (mp-1634) <1 1 0> <0 0 1> 0.171 264.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
281 75 97 0 0 0
75 281 97 0 0 0
97 97 283 0 0 0
0 0 0 114 0 0
0 0 0 0 114 0
0 0 0 0 0 103
Compliance Tensor Sij (10-12Pa-1)
4.2 -0.7 -1.2 0 0 0
-0.7 4.2 -1.2 0 0 0
-1.2 -1.2 4.3 0 0 0
0 0 0 8.7 0 0
0 0 0 0 8.7 0
0 0 0 0 0 9.7
Shear Modulus GV
105 GPa
Bulk Modulus KV
154 GPa
Shear Modulus GR
104 GPa
Bulk Modulus KR
153 GPa
Shear Modulus GVRH
104 GPa
Bulk Modulus KVRH
153 GPa
Elastic Anisotropy
0.05
Poisson's Ratio
0.22

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ta2GaC (mp-1025427) 0.1298 0.000 3
Cr2SiC (mp-1078494) 0.1146 0.118 3
Nb2GaC (mp-1079546) 0.0858 0.000 3
GaMo2C (mp-1079635) 0.1061 0.006 3
Ti2SiC (mp-1079908) 0.1003 0.018 3
Ti2O (mp-1215) 0.7468 0.000 2
Co3H (mp-1025425) 0.6376 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ti_pv Ge_d C
Final Energy/Atom
-8.2196 eV
Corrected Energy
-65.7568 eV
-65.7568 eV = -65.7568 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 180769
  • 42921
Submitted by
User remarks:
  • Titanium germanium carbide (2/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)