Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNon-magnetic |
Formation Energy / Atom-1.016 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.026 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.41 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToKAgO2 |
Band Gap0.600 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPmmm [47] |
Hall-P 2 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 122.9 |
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 238.5 |
LaAlO3 (mp-2920) | <1 1 1> | <1 1 1> | 122.9 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 144.6 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 45.4 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 34.1 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 193.1 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 198.8 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 277.5 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 221.2 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 238.5 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 170.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 287.5 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 238.5 |
GaAs (mp-2534) | <1 1 1> | <0 1 1> | 170.7 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 162.6 |
BaF2 (mp-1029) | <1 1 1> | <0 1 0> | 271.0 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 223.8 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 57.1 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 234.8 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 149.2 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 170.7 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 159.0 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 198.8 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 199.1 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 159.0 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 85.4 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 248.6 |
KCl (mp-23193) | <1 0 0> | <1 1 1> | 122.9 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 238.5 |
KCl (mp-23193) | <1 1 1> | <0 1 0> | 271.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 216.8 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 159.0 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 272.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 216.8 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 238.5 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 318.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 113.6 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 159.0 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 271.0 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 284.0 |
ZnSe (mp-1190) | <1 1 1> | <0 1 1> | 170.7 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 287.5 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 1> | 223.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 144.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 213.4 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 176.9 |
CdS (mp-672) | <1 0 0> | <0 1 1> | 149.4 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 49.7 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 193.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points32 |
U Values-- |
PseudopotentialsVASP PAW: K_sv Ag O |
Final Energy/Atom-4.1153 eV |
Corrected Energy-17.8659 eV
-17.8659 eV = -16.4613 eV (uncorrected energy) - 1.4046 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)