Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.158 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.003 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.70 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAg5BiO4 + Bi2O3 |
Band Gap1.668 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 337.9 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 285.1 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 193.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 217.9 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 193.7 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 217.9 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 239.6 |
CeO2 (mp-20194) | <1 0 0> | <1 0 -1> | 239.6 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 289.6 |
GaAs (mp-2534) | <1 0 0> | <0 1 1> | 337.9 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 334.0 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 290.3 |
BaF2 (mp-1029) | <1 0 0> | <0 1 1> | 241.3 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 217.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 193.7 |
GaN (mp-804) | <1 0 0> | <1 0 -1> | 186.4 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 241.9 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 145.3 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 122.2 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 193.7 |
SiO2 (mp-6930) | <1 1 0> | <1 1 1> | 291.6 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 241.3 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 219.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 122.2 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 217.9 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 1> | 289.6 |
InAs (mp-20305) | <1 0 0> | <1 1 0> | 338.7 |
InAs (mp-20305) | <1 1 1> | <1 0 -1> | 319.5 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 334.0 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 290.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 314.8 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 314.8 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 314.8 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 121.1 |
YVO4 (mp-19133) | <0 0 1> | <1 0 -1> | 53.2 |
YVO4 (mp-19133) | <1 0 0> | <1 0 -1> | 186.4 |
YVO4 (mp-19133) | <1 0 1> | <1 0 -1> | 213.0 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 193.5 |
YVO4 (mp-19133) | <1 1 1> | <0 0 1> | 169.5 |
Te2Mo (mp-602) | <0 0 1> | <1 0 -1> | 133.1 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 219.9 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 167.0 |
GaSe (mp-1943) | <1 1 0> | <0 0 1> | 121.1 |
BN (mp-984) | <1 0 0> | <1 0 -1> | 292.9 |
BN (mp-984) | <1 0 1> | <1 1 -1> | 247.6 |
BN (mp-984) | <1 1 1> | <0 1 1> | 241.3 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 1> | 291.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 -1> | 106.5 |
Al (mp-134) | <1 0 0> | <1 0 -1> | 213.0 |
Al (mp-134) | <1 1 0> | <0 1 0> | 167.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BiAuO2 (mp-997082) | 0.3245 | 0.038 | 3 |
CuBiO2 (mp-997054) | 0.3330 | 0.010 | 3 |
AgBiO2 (mp-996970) | 0.5301 | 0.026 | 3 |
Hg5(ClO2)2 (mp-23358) | 0.5517 | 0.000 | 3 |
Hg5(BrO2)2 (mp-23543) | 0.5526 | 0.000 | 3 |
Th2Fe2Si2C (mp-1025382) | 0.7414 | 0.000 | 4 |
SnHg2(SBr)2 (mp-643460) | 0.6760 | 0.000 | 4 |
La2Fe(SeO)2 (mp-1078132) | 0.7347 | 0.000 | 4 |
Ce2Fe(SeO)2 (mp-1078159) | 0.7166 | 0.007 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ag Bi O |
Final Energy/Atom-4.9613 eV |
Corrected Energy-42.4996 eV
-42.4996 eV = -39.6905 eV (uncorrected energy) - 2.8092 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)