Final Magnetic Moment0.061 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.581 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.012 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.86 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAu2O3 + Au + PdO |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 176.2 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 231.8 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 122.8 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 370.9 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 111.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 259.6 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 148.4 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 194.7 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 64.9 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 166.9 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 138.2 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 176.2 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 9.3 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 119.6 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 39.9 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 157.6 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 148.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 64.9 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 139.1 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 148.4 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 207.2 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 138.2 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 287.5 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 296.7 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 296.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 138.2 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 55.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 92.7 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 361.6 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 64.9 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 194.7 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 207.2 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 166.9 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 176.2 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 138.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 176.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 69.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 27.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 64.9 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 199.4 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 239.3 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 324.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 83.5 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 69.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 27.8 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 159.5 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 259.6 |
YVO4 (mp-19133) | <1 1 0> | <1 0 1> | 327.6 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 185.5 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 176.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
PdAuO2 (mp-997051) | 0.1601 | 0.013 | 3 |
CuBrO2 (mp-1096943) | 0.0111 | 0.041 | 3 |
LuAgO2 (mp-1018025) | 0.0585 | 0.000 | 3 |
ScAuO2 (mp-11023) | 0.0610 | 0.012 | 3 |
InAuO2 (mp-19723) | 0.1410 | 0.016 | 3 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pd Au O |
Final Energy/Atom-4.8173 eV |
Corrected Energy-41.3475 eV
-41.3475 eV = -38.5383 eV (uncorrected energy) - 2.8092 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)