material

SrAgO2

ID:

mp-997100

DOI:

10.17188/1317183


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.826 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.011 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.09 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
SrAgO2
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4/mcm [140]
Hall
-I 4 2c
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
TiO2 (mp-390) <0 0 1> <0 0 1> 0.001 72.4
MgO (mp-1265) <1 0 0> <0 0 1> 0.002 36.2
Al2O3 (mp-1143) <1 0 1> <1 0 0> 0.006 330.1
Mg (mp-153) <1 0 0> <1 1 0> 0.012 116.7
ZnO (mp-2133) <1 0 1> <0 0 1> 0.013 217.1
PbS (mp-21276) <1 0 0> <0 0 1> 0.013 36.2
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.013 144.7
GaN (mp-804) <1 1 1> <1 0 1> 0.015 274.4
KCl (mp-23193) <1 0 0> <1 0 1> 0.032 164.6
Fe3O4 (mp-19306) <1 0 0> <0 0 1> 0.033 72.4
LiAlO2 (mp-3427) <1 0 0> <1 1 0> 0.043 233.4
NaCl (mp-22862) <1 0 0> <0 0 1> 0.044 289.4
TiO2 (mp-2657) <1 1 0> <0 0 1> 0.047 253.3
CdWO4 (mp-19387) <0 0 1> <1 0 0> 0.047 123.8
LiNbO3 (mp-3731) <0 0 1> <1 0 0> 0.048 165.1
PbS (mp-21276) <1 1 0> <1 0 0> 0.051 206.3
MgF2 (mp-1249) <1 1 1> <1 0 0> 0.053 330.1
CdWO4 (mp-19387) <1 0 0> <1 0 0> 0.054 123.8
ZnO (mp-2133) <1 0 0> <1 1 0> 0.057 175.1
Mg (mp-153) <0 0 1> <1 0 0> 0.058 165.1
KCl (mp-23193) <1 1 0> <1 0 0> 0.062 288.8
ZnO (mp-2133) <1 1 0> <1 1 1> 0.073 274.6
ZrO2 (mp-2858) <1 1 1> <1 0 0> 0.074 206.3
LiTaO3 (mp-3666) <0 0 1> <1 0 0> 0.076 165.1
MgO (mp-1265) <1 1 1> <1 0 0> 0.081 123.8
LiGaO2 (mp-5854) <0 1 1> <1 1 0> 0.083 175.1
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.088 165.1
WS2 (mp-224) <0 0 1> <1 0 0> 0.088 165.1
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.089 144.7
MgO (mp-1265) <1 1 0> <0 0 1> 0.092 180.9
GaSe (mp-1943) <0 0 1> <1 0 0> 0.094 165.1
CdS (mp-672) <1 1 0> <1 0 0> 0.102 247.6
YAlO3 (mp-3792) <0 1 0> <1 1 1> 0.102 274.6
YAlO3 (mp-3792) <1 1 1> <1 0 0> 0.103 123.8
YAlO3 (mp-3792) <0 1 1> <1 0 0> 0.104 288.8
Cu (mp-30) <1 0 0> <1 1 0> 0.122 291.8
CdS (mp-672) <1 0 0> <1 1 0> 0.135 58.4
C (mp-48) <0 0 1> <1 0 0> 0.138 165.1
BaTiO3 (mp-5986) <1 1 0> <1 1 0> 0.141 291.8
NaCl (mp-22862) <1 1 1> <1 0 0> 0.142 165.1
BaTiO3 (mp-5986) <1 0 0> <1 1 1> 0.144 68.7
NdGaO3 (mp-3196) <0 0 1> <1 1 1> 0.147 274.6
Bi2Se3 (mp-541837) <1 0 0> <0 0 1> 0.166 253.3
TeO2 (mp-2125) <0 0 1> <0 0 1> 0.172 289.4
Al (mp-134) <1 0 0> <0 0 1> 0.173 144.7
YAlO3 (mp-3792) <1 0 1> <1 0 0> 0.178 288.8
GdScO3 (mp-5690) <1 1 0> <0 0 1> 0.179 325.6
WS2 (mp-224) <1 0 1> <1 0 1> 0.194 274.4
Te2W (mp-22693) <0 0 1> <1 1 0> 0.201 175.1
YVO4 (mp-19133) <1 0 0> <1 0 0> 0.220 330.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
237 103 17 0 0 0
103 237 17 0 0 0
17 17 91 0 0 0
0 0 0 17 0 0
0 0 0 0 17 0
0 0 0 0 0 52
Compliance Tensor Sij (10-12Pa-1)
5.2 -2.2 -0.5 0 0 0
-2.2 5.2 -0.5 0 0 0
-0.5 -0.5 11.2 0 0 0
0 0 0 58.6 0 0
0 0 0 0 58.6 0
0 0 0 0 0 19.4
Shear Modulus GV
46 GPa
Bulk Modulus KV
93 GPa
Shear Modulus GR
29 GPa
Bulk Modulus KR
67 GPa
Shear Modulus GVRH
38 GPa
Bulk Modulus KVRH
80 GPa
Elastic Anisotropy
3.17
Poisson's Ratio
0.30

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
CaFeO2 (mvc-16214) 0.3155 0.091 3
CaCuS2 (mp-1096857) 0.3378 0.186 3
NdNiO2 (mp-542468) 0.3369 0.431 3
CaFeO2 (mp-24946) 0.3026 0.091 3
LiPH2 (mp-1094124) 0.3203 0.369 3
Ba2Pd(OF)2 (mp-6123) 0.7481 0.052 4
Ca3Cu2(BrO2)2 (mp-545706) 0.7296 0.001 4
CO3 (mp-995196) 0.4184 3.070 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Sr_sv Ag O
Final Energy/Atom
-5.0797 eV
Corrected Energy
-43.4469 eV
-43.4469 eV = -40.6378 eV (uncorrected energy) - 2.8092 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)