Final Magnetic Moment4.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.384 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.87 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <1 1 1> | 318.2 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 1> | 257.2 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 1> | 257.2 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 141.4 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 286.9 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 57.4 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 200.1 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 281.3 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 172.1 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 95.6 |
AlN (mp-661) | <1 0 1> | <1 0 -1> | 112.4 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 206.3 |
CeO2 (mp-20194) | <1 0 0> | <1 0 -1> | 292.3 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 172.1 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 223.5 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 137.5 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 292.2 |
GaN (mp-804) | <0 0 1> | <1 1 -1> | 125.7 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 117.9 |
GaN (mp-804) | <1 0 1> | <1 0 -1> | 112.4 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 120.3 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 153.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 275.0 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 141.4 |
SiO2 (mp-6930) | <1 0 1> | <1 1 -1> | 251.3 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 200.1 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 153.0 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 248.6 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 57.4 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 286.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 154.7 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 172.1 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 314.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 137.5 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 -1> | 112.4 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 1> | 314.4 |
DyScO3 (mp-31120) | <1 1 1> | <1 1 1> | 136.4 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 38.2 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 267.7 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 257.8 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 223.5 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 137.5 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 292.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 212.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 68.8 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 -1> | 112.4 |
CdS (mp-672) | <0 0 1> | <1 0 -1> | 157.4 |
CdS (mp-672) | <1 0 0> | <1 1 1> | 90.9 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 160.7 |
CdS (mp-672) | <1 1 0> | <1 0 -1> | 157.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BaCa4(CoN2)2 (mvc-16412) | 0.7150 | 0.000 | 4 |
Sr2BN2F (mp-10234) | 0.7462 | 0.000 | 4 |
Ca2BN2F (mp-10233) | 0.7485 | 0.000 | 4 |
BaCa4(CoN2)2 (mp-606338) | 0.7230 | 0.000 | 4 |
MnAgO2 (mp-996995) | 0.0988 | 0.000 | 3 |
AgBiO2 (mp-996970) | 0.6088 | 0.026 | 3 |
PbAuO2 (mp-997014) | 0.6521 | 0.026 | 3 |
MnCuO2 (mp-510589) | 0.1890 | 0.000 | 3 |
TiCu3O4 (mp-758229) | 0.5736 | 0.074 | 3 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-points128 |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Mn_pv Au O |
Final Energy/Atom-6.1884 eV |
Corrected Energy-27.8390 eV
-27.8390 eV = -24.7536 eV (uncorrected energy) - 1.6809 eV (MP Advanced Correction) - 1.4046 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)