Final Magnetic Moment13.048 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.671 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.027 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.25 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFe3(P2O7)2 + Ti2Fe(PO5)2 + VPO4 |
Band Gap0.060 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [146] |
HallR 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 195.7 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 195.7 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 65.2 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 326.1 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 260.9 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 65.2 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 260.9 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 326.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 195.7 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 195.7 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 260.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 65.2 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 326.1 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 191.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 260.9 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 260.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 195.7 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 260.9 |
BN (mp-984) | <0 0 1> | <0 0 1> | 65.2 |
BN (mp-984) | <1 1 0> | <0 0 1> | 65.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 195.7 |
Al (mp-134) | <1 1 1> | <0 0 1> | 195.7 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 195.7 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 130.4 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 180.0 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 195.7 |
C (mp-66) | <1 1 1> | <0 0 1> | 65.2 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 326.1 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 326.1 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 65.2 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 260.9 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 65.2 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 65.2 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 65.2 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 260.9 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 326.1 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 260.9 |
PbSe (mp-2201) | <1 0 0> | <1 0 1> | 191.5 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 1> | 191.5 |
MoSe2 (mp-1634) | <1 1 0> | <0 0 1> | 260.9 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 260.9 |
Si (mp-149) | <1 1 0> | <0 0 1> | 326.1 |
Si (mp-149) | <1 1 1> | <0 0 1> | 195.7 |
Au (mp-81) | <1 1 1> | <0 0 1> | 260.9 |
WSe2 (mp-1821) | <1 1 0> | <0 0 1> | 260.9 |
WSe2 (mp-1821) | <1 1 1> | <0 0 1> | 260.9 |
CdSe (mp-2691) | <1 0 0> | <1 0 1> | 191.5 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 65.2 |
C (mp-48) | <0 0 1> | <0 0 1> | 195.7 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 260.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnPO4 (mp-773411) | 0.1980 | 0.344 | 3 |
VPO4 (mp-861584) | 0.1230 | 0.079 | 3 |
MnCrO4 (mp-769911) | 0.4336 | 0.073 | 3 |
FePO4 (mp-773675) | 0.3617 | 0.045 | 3 |
TiPO4 (mp-779587) | 0.1873 | 0.077 | 3 |
VFe(PO4)2 (mp-770962) | 0.0702 | 0.015 | 4 |
V5Cr(PO4)6 (mp-770858) | 0.1021 | 0.068 | 4 |
TiV(PO4)2 (mp-850923) | 0.0822 | 0.002 | 4 |
V2Co(PO4)3 (mp-772401) | 0.0959 | 0.161 | 4 |
Ti2Fe(PO4)3 (mp-778242) | 0.1039 | 0.101 | 4 |
Mo4O11 (mp-565865) | 0.7320 | 0.026 | 2 |
VO2 (mvc-6918) | 0.7347 | 0.095 | 2 |
MoO2 (mvc-6944) | 0.6993 | 0.281 | 2 |
Ti3CrNi2(PO4)6 (mp-777498) | 0.0720 | 0.197 | 5 |
Ti3CrFe2(PO4)6 (mp-776921) | 0.0528 | 0.726 | 5 |
TiFe3Cu2(PO4)6 (mp-775996) | 0.0697 | 0.053 | 5 |
TiZnCr(PO4)3 (mvc-9198) | 0.0791 | 0.011 | 5 |
TiVZn(PO4)3 (mvc-9187) | 0.0777 | 0.101 | 5 |
Na2Li3Ti3Al(PO4)6 (mp-769078) | 0.5266 | 0.068 | 6 |
LiTi3MnCr(PO4)6 (mp-772224) | 0.2428 | 0.001 | 6 |
Li2Ti2MnCr2(PO4)6 (mp-777244) | 0.4692 | 0.015 | 6 |
Na2LiTi3Al(PO4)6 (mp-769074) | 0.5443 | 0.011 | 6 |
Na2LiTi3Al(PO4)6 (mp-769073) | 0.5285 | 0.014 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eVFe: 5.3 eV |
PseudopotentialsVASP PAW: Ti_pv V_pv Fe_pv P O |
Final Energy/Atom-7.5584 eV |
Corrected Energy-299.4681 eV
-299.4681 eV = -272.1011 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 10.5120 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)