Final Magnetic Moment5.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.365 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.028 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.74 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiFePO4 + Li2CuP2O7 + CuO |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 243.9 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 0> | 231.9 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 142.5 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 142.5 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 256.6 |
CdS (mp-672) | <1 1 0> | <1 1 1> | 248.6 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 313.6 |
LiF (mp-1138) | <1 1 1> | <1 1 0> | 231.9 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 285.0 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 304.9 |
TePb (mp-19717) | <1 1 1> | <0 1 1> | 221.6 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 228.1 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 142.5 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 85.5 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 182.9 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 182.9 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 142.5 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 171.1 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 61.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 199.6 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 114.0 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 231.9 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 203.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 1> | 277.0 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 231.9 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 304.9 |
GaSe (mp-1943) | <1 0 0> | <0 1 1> | 277.0 |
BaF2 (mp-1029) | <1 1 1> | <0 1 1> | 277.0 |
BN (mp-984) | <0 0 1> | <0 0 1> | 114.0 |
BN (mp-984) | <1 0 0> | <1 1 0> | 77.3 |
BN (mp-984) | <1 0 1> | <0 0 1> | 313.6 |
BN (mp-984) | <1 1 0> | <0 0 1> | 228.1 |
BN (mp-984) | <1 1 1> | <0 1 0> | 237.5 |
LiNbO3 (mp-3731) | <1 1 0> | <0 0 1> | 256.6 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 332.4 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 182.9 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 135.8 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 271.5 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 332.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 1> | 277.0 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 309.2 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 142.5 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 332.4 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 271.5 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 256.6 |
Al (mp-134) | <1 0 0> | <1 0 0> | 243.9 |
Al (mp-134) | <1 1 1> | <1 1 0> | 231.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 271.5 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 332.4 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 114.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Zn2SiO4 (mp-1020609) | 0.2816 | 0.083 | 3 |
Co2SiO4 (mp-555558) | 0.2826 | 0.617 | 3 |
Mn2SiO4 (mp-18928) | 0.2419 | 0.000 | 3 |
Fe2SiO4 (mp-510587) | 0.2464 | 0.000 | 3 |
Ca2GeO4 (mp-560647) | 0.2916 | 0.000 | 3 |
Li3Mn(PO4)2 (mp-771633) | 0.1838 | 0.020 | 4 |
LiFePO4 (mp-761468) | 0.1945 | 0.056 | 4 |
Li3Fe(PO4)2 (mp-773399) | 0.1604 | 0.012 | 4 |
LiCrPO4 (mp-25507) | 0.1951 | 0.547 | 4 |
LiCuPO4 (mp-25449) | 0.1906 | 0.035 | 4 |
Fe3O4 (mp-715491) | 0.6777 | 0.017 | 2 |
Mn3N4 (mp-1080204) | 0.6771 | 0.172 | 2 |
Cr3N4 (mp-1014358) | 0.5964 | 0.227 | 2 |
Fe3O4 (mp-650112) | 0.6490 | 0.060 | 2 |
Fe3O4 (mp-716052) | 0.6768 | 0.781 | 2 |
Li4CuNi3(PO4)4 (mp-767664) | 0.1015 | 0.014 | 5 |
Li2CrNi(PO4)2 (mp-761997) | 0.1041 | 0.047 | 5 |
Li2CuNi(PO4)2 (mp-767151) | 0.0814 | 0.021 | 5 |
Li2CrCo(PO4)2 (mp-761707) | 0.1072 | 0.035 | 5 |
Li4CoCu3(PO4)4 (mp-761537) | 0.0744 | 0.108 | 5 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.1790 | 0.014 | 6 |
Li3MnFeCo(PO4)3 (mp-764708) | 0.1808 | 0.599 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.1850 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764707) | 0.1842 | 0.035 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.1848 | 0.466 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv Cu_pv P O |
Final Energy/Atom-6.5393 eV |
Corrected Energy-199.8036 eV
-199.8036 eV = -183.1010 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 5.4660 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)