Final Magnetic Moment6.768 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.329 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.077 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.83 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiNiO2 + Fe2NiO4 + Li(NiO2)2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 287.4 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 199.0 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 353.7 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 265.3 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 353.7 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 221.1 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 309.5 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 243.2 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 154.8 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 199.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 353.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 353.7 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 176.9 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 309.5 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 132.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 199.0 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 265.3 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 199.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 287.4 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 287.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 22.1 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 265.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 353.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 353.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 309.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 88.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 199.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 353.7 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 88.4 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 265.3 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 287.4 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 88.4 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 88.4 |
BN (mp-984) | <1 0 0> | <0 0 1> | 154.8 |
LiNbO3 (mp-3731) | <1 0 0> | <1 -1 0> | 146.3 |
Al (mp-134) | <1 1 1> | <0 0 1> | 88.4 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 309.5 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 221.1 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 199.0 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 265.3 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 353.7 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 331.6 |
LiTaO3 (mp-3666) | <1 0 1> | <1 0 0> | 146.0 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 154.8 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 199.0 |
C (mp-66) | <1 0 0> | <0 0 1> | 221.1 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 353.7 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 287.4 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 331.6 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 265.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3Fe7O12 (mp-762465) | 0.1716 | 0.107 | 3 |
Li5Fe5O12 (mp-762602) | 0.1611 | 0.694 | 3 |
Li3V7O12 (mp-762285) | 0.1330 | 0.078 | 3 |
Li5V5O12 (mp-762939) | 0.1803 | 0.156 | 3 |
Li3Cr2Fe5O12 (mp-780009) | 0.1931 | 0.967 | 4 |
Li3Fe5(CoO6)2 (mp-773618) | 0.1710 | 0.118 | 4 |
Li3Mn2Ni5O12 (mp-762611) | 0.1822 | 0.061 | 4 |
Li2Mn(FeO3)2 (mp-762835) | 0.1503 | 0.071 | 4 |
Li2Fe2CuO6 (mp-849448) | 0.1272 | 0.075 | 4 |
Ni6O7 (mp-767815) | 0.2323 | 0.047 | 2 |
Ni5O6 (mp-782702) | 0.3029 | 0.041 | 2 |
V6C5 (mp-28731) | 0.2751 | 0.000 | 2 |
Fe7O8 (mp-715333) | 0.3108 | 0.064 | 2 |
Ni6Cl7 (mp-1022720) | 0.2632 | 0.167 | 2 |
Li6Mn3Cr2Fe3O16 (mp-861553) | 0.4130 | 0.882 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eVNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv Ni_pv O |
Final Energy/Atom-5.2482 eV |
Corrected Energy-422.7631 eV
Uncorrected energy = -346.3801 eV
Composition-based energy adjustment (-0.687 eV/atom x 36.0 atoms) = -24.7320 eV
Composition-based energy adjustment (-2.256 eV/atom x 6.0 atoms) = -13.5360 eV
Composition-based energy adjustment (-2.541 eV/atom x 15.0 atoms) = -38.1150 eV
Corrected energy = -422.7631 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)