Final Magnetic Moment12.007 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.379 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.219 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.44 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiFePO4 + FeF2 + LiF |
Band Gap3.321 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63 [173] |
HallP 6c |
Point Group6 |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 174.3 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 151.0 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 174.3 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 261.5 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 87.2 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 261.5 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 174.3 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 261.5 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 174.3 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 261.5 |
Mg (mp-153) | <1 0 1> | <1 1 0> | 151.0 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 160.1 |
InSb (mp-20012) | <1 1 0> | <1 0 0> | 261.5 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 174.3 |
PbSe (mp-2201) | <1 1 0> | <1 0 0> | 174.3 |
C (mp-48) | <0 0 1> | <1 0 0> | 174.3 |
ZnO (mp-2133) | <0 0 1> | <1 0 0> | 261.5 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 160.1 |
LiAlO2 (mp-3427) | <1 0 0> | <1 0 0> | 261.5 |
CaF2 (mp-2741) | <1 1 1> | <0 0 1> | 160.1 |
Fe2O3 (mp-24972) | <0 0 1> | <0 0 1> | 160.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Co3(PO4)2 (mp-651271) | 0.4445 | 0.016 | 3 |
Fe4P2O9 (mp-637226) | 0.4589 | 0.391 | 3 |
Mn4P2O9 (mp-770499) | 0.4511 | 0.015 | 3 |
Li2SO4 (mp-558382) | 0.4559 | 0.055 | 3 |
Ni4P2O9 (mp-771899) | 0.4368 | 0.037 | 3 |
Li3Mo(PO4)2 (mp-32100) | 0.3229 | 0.025 | 4 |
Li3Sb(PO4)2 (mp-758533) | 0.3221 | 0.081 | 4 |
Li3P2WO8 (mp-763373) | 0.3142 | 0.046 | 4 |
Li3Ti(PO4)2 (mp-758151) | 0.2978 | 0.070 | 4 |
Li3Ti(PO4)2 (mp-757905) | 0.3465 | 0.072 | 4 |
Li7Mn7P6(O8F)3 (mp-763896) | 0.1051 | 0.022 | 5 |
Li7V7P6(O8F)3 (mp-763895) | 0.1669 | 0.131 | 5 |
Na3LiSbP2O9 (mp-761144) | 0.4612 | 0.081 | 5 |
Li4V2Si(PO6)2 (mp-770404) | 0.4503 | 0.077 | 5 |
Li7Cr7P6(O8F)3 (mp-763893) | 0.2523 | 0.510 | 5 |
Li2VCrP2(HO5)2 (mp-767127) | 0.6914 | 0.050 | 6 |
Li2VCrP2(HO5)2 (mp-767007) | 0.6981 | 0.048 | 6 |
Li3MnVP2(O4F)2 (mp-763904) | 0.6872 | 0.034 | 6 |
Li3VCrP2(O4F)2 (mp-766992) | 0.6468 | 0.027 | 6 |
Li2Mg2MnFe(PO4)4 (mp-849669) | 0.6565 | 0.008 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv P O F |
Final Energy/Atom-6.4672 eV |
Corrected Energy-679.8851 eV
-679.8851 eV = -607.9132 eV (uncorrected energy) - 38.2620 eV (MP Advanced Correction) - 33.7099 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)