Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.164 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.041 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.87 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToRbInBr4 + RbBr + InBr |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 329.0 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 232.4 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 197.4 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 263.1 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 65.8 |
BaF2 (mp-1029) | <1 0 0> | <1 1 0> | 328.9 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 46.5 |
GaAs (mp-2534) | <1 1 1> | <0 1 0> | 232.4 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 197.3 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 232.4 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 263.1 |
SiO2 (mp-6930) | <1 0 0> | <1 1 1> | 279.3 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 139.4 |
KCl (mp-23193) | <1 0 0> | <1 1 0> | 328.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 93.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 131.6 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 161.1 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 46.5 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 65.8 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 329.0 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 65.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 46.5 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 278.9 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 46.5 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 232.4 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 65.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 232.4 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 325.4 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 263.2 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 232.4 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 65.8 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 46.5 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 232.4 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 278.9 |
YVO4 (mp-19133) | <0 0 1> | <1 1 0> | 263.1 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 185.9 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 241.7 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 139.4 |
TePb (mp-19717) | <1 0 0> | <1 1 0> | 328.9 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 241.7 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 232.4 |
BN (mp-984) | <0 0 1> | <0 1 0> | 325.4 |
BN (mp-984) | <1 0 1> | <0 1 0> | 185.9 |
BN (mp-984) | <1 1 0> | <0 1 0> | 325.4 |
BN (mp-984) | <1 1 1> | <0 1 0> | 232.4 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 185.9 |
BN (mp-984) | <1 0 0> | <1 1 0> | 197.3 |
MoS2 (mp-1434) | <0 0 1> | <1 1 0> | 328.9 |
Al (mp-134) | <1 1 0> | <0 1 0> | 46.5 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 131.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CsCaI3 (mp-998333) | 0.0317 | 0.021 | 3 |
RbCaBr3 (mp-998198) | 0.0285 | 0.024 | 3 |
RbAgBr3 (mp-998212) | 0.0463 | 0.000 | 3 |
RbCaCl3 (mp-998197) | 0.0382 | 0.010 | 3 |
SrNiO3 (mp-762506) | 0.0408 | 0.040 | 3 |
Sr2FeWO6 (mp-555520) | 0.0811 | 0.204 | 4 |
LaSm(CoO3)2 (mp-1075930) | 0.1423 | 0.094 | 4 |
K5Na3Nb8O24 (mp-1076335) | 0.1379 | 0.024 | 4 |
LaSm(NiO3)2 (mp-1076325) | 0.1370 | 0.081 | 4 |
SrCa3Mn4O12 (mp-1076020) | 0.1408 | 0.103 | 4 |
Mn4N (mp-637576) | 0.1721 | 1.987 | 2 |
Fe2O3 (mp-1068212) | 0.1831 | 0.860 | 2 |
Fe4P (mp-20885) | 0.1936 | 0.695 | 2 |
Ni4O (mp-1094082) | 0.1937 | 1.616 | 2 |
Ni4N (mp-1094090) | 0.1937 | 0.067 | 2 |
La5Sm3Co7CuO24 (mp-1076171) | 0.0994 | 0.105 | 5 |
La3SmV2Cr2O12 (mp-1076218) | 0.1051 | 0.132 | 5 |
Sr5Ca3Mn4(FeO6)4 (mp-1076796) | 0.1039 | 0.050 | 5 |
Sr5Ca3Ti3Mn5O24 (mp-1075962) | 0.0983 | 0.052 | 5 |
Sr5Ca3TiMn7O24 (mp-1075976) | 0.1070 | 0.068 | 5 |
Na5Ca2Ce3Ti8Nb2O30 (mp-721094) | 0.6497 | 0.065 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Rb_sv In_d Br |
Final Energy/Atom-2.8926 eV |
Corrected Energy-14.4631 eV
-14.4631 eV = -14.4631 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)