Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.775 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.004 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.42 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSeBr4 + RbBr + Se |
Band Gap1.302 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 316.6 |
AlN (mp-661) | <1 0 0> | <1 1 1> | 202.5 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 297.6 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 135.5 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 297.6 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 207.4 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 263.8 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 316.6 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 163.5 |
BaF2 (mp-1029) | <1 1 1> | <1 1 -1> | 276.4 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 207.4 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 297.6 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 170.1 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 211.0 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 297.6 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 135.5 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 255.1 |
SiO2 (mp-6930) | <1 1 0> | <1 0 -1> | 245.2 |
KCl (mp-23193) | <1 0 0> | <1 0 -1> | 81.7 |
KCl (mp-23193) | <1 1 0> | <1 1 -1> | 276.4 |
KCl (mp-23193) | <1 1 1> | <1 1 -1> | 276.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 158.3 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 271.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 316.6 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 212.6 |
InAs (mp-20305) | <1 1 0> | <1 0 -1> | 163.5 |
InAs (mp-20305) | <1 1 1> | <1 1 -1> | 276.4 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 263.8 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 316.6 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 81.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 158.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 1> | 203.3 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 316.6 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 297.6 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 207.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 263.8 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 211.0 |
LiF (mp-1138) | <1 1 1> | <0 1 1> | 203.3 |
Te2W (mp-22693) | <0 0 1> | <1 0 -1> | 245.2 |
Te2W (mp-22693) | <1 0 0> | <0 1 1> | 203.3 |
Te2W (mp-22693) | <1 0 1> | <0 1 1> | 203.3 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 263.8 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 183.8 |
Te2Mo (mp-602) | <0 0 1> | <1 0 -1> | 163.5 |
Te2Mo (mp-602) | <1 0 0> | <1 1 -1> | 276.4 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 276.5 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 -1> | 245.2 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 -1> | 245.2 |
Ag (mp-124) | <1 1 0> | <1 0 -1> | 245.2 |
Ag (mp-124) | <1 1 1> | <0 1 1> | 203.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CsSeBr3 (mp-998413) | 0.2003 | 0.003 | 3 |
Sr2Cu2SbO7 (mvc-273) | 0.7379 | 0.287 | 4 |
Sr2Cu2TeO7 (mvc-274) | 0.7312 | 0.308 | 4 |
KICl2O (mp-1080792) | 0.7413 | 0.106 | 4 |
Au3F8 (mp-17407) | 0.7159 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Rb_sv Se Br |
Final Energy/Atom-2.6528 eV |
Corrected Energy-26.5285 eV
-26.5285 eV = -26.5285 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)