Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.731 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.009 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.71 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTa2Se + TaSe2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Topological ClassificationTI*
|
SubclassificationNLC†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
InAs (mp-20305) | <1 0 0> | <1 0 0> | 351.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 68.5 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 -1> | 171.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 272.6 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 87.1 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 221.9 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 255.3 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 159.0 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 255.3 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 255.3 |
LiF (mp-1138) | <1 1 1> | <1 0 -1> | 171.3 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 43.5 |
Te2W (mp-22693) | <0 1 0> | <1 0 -1> | 102.8 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 113.6 |
YVO4 (mp-19133) | <0 0 1> | <1 0 -1> | 102.8 |
YVO4 (mp-19133) | <1 1 0> | <1 0 1> | 130.6 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 179.3 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 181.7 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 272.6 |
Te2Mo (mp-602) | <1 1 0> | <1 1 -1> | 275.6 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 255.3 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 272.6 |
Ag (mp-124) | <1 1 1> | <1 0 -1> | 239.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 1> | 255.8 |
GaSe (mp-1943) | <0 0 1> | <1 0 -1> | 171.3 |
BN (mp-984) | <0 0 1> | <0 0 1> | 181.7 |
BN (mp-984) | <1 0 0> | <1 0 -1> | 171.3 |
BN (mp-984) | <1 0 1> | <1 0 -1> | 239.8 |
BN (mp-984) | <1 1 1> | <0 1 0> | 239.1 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 95.7 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 -1> | 342.6 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 217.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 249.9 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 203.3 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 223.4 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 217.7 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 319.1 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 127.6 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 272.6 |
GaAs (mp-2534) | <1 1 0> | <1 0 -1> | 137.1 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 272.6 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 351.0 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 179.3 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 68.2 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 159.0 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 204.5 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 249.9 |
SiO2 (mp-6930) | <0 0 1> | <1 0 -1> | 171.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 136.3 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 287.2 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
148 | 68 | 65 | 0 | -20 | 0 |
68 | 159 | 51 | 0 | -11 | 0 |
65 | 51 | 104 | 0 | -20 | 0 |
0 | 0 | 0 | 47 | 0 | -17 |
-20 | -11 | -20 | 0 | 52 | 0 |
0 | 0 | 0 | -17 | 0 | 55 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
10.3 | -2.8 | -4.8 | 0 | 1.5 | 0 |
-2.8 | 8.2 | -2.4 | 0 | -0.2 | 0 |
-4.8 | -2.4 | 14.5 | 0 | 3.2 | 0 |
0 | 0 | 0 | 23.6 | 0 | 7.1 |
1.5 | -0.2 | 3.2 | 0 | 20.9 | 0 |
0 | 0 | 0 | 7.1 | 0 | 20.2 |
Shear Modulus GV46 GPa |
Bulk Modulus KV86 GPa |
Shear Modulus GR41 GPa |
Bulk Modulus KR76 GPa |
Shear Modulus GVRH44 GPa |
Bulk Modulus KVRH81 GPa |
Elastic Anisotropy0.76 |
Poisson's Ratio0.27 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Nb2VSe4 (mp-1025195) | 0.7308 | 0.006 | 3 |
Y3RuI3 (mp-28747) | 0.6905 | 0.000 | 3 |
Ga3B4Pt9 (mp-28869) | 0.7200 | 0.000 | 3 |
Tl4SnSe3 (mp-531170) | 0.7130 | 0.000 | 3 |
V(FeSe2)2 (mp-1078113) | 0.6626 | 0.080 | 3 |
RbHfAgTe3 (mp-9780) | 0.4862 | 0.000 | 4 |
V3Se4 (mp-990764) | 0.7213 | 0.000 | 2 |
Ti3Te4 (mp-15669) | 0.6575 | 0.000 | 2 |
Nb2Te3 (mp-570451) | 0.6861 | 0.039 | 2 |
Nb2Se3 (mp-2330) | 0.0945 | 0.017 | 2 |
Mo2S3 (mp-1627) | 0.4036 | 0.096 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ta_pv Se |
Final Energy/Atom-7.5721 eV |
Corrected Energy-75.7210 eV
-75.7210 eV = -75.7210 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)