Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingUnknown |
Formation Energy / Atom-0.821 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.001 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.84 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSnS2 |
Band Gap1.486 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63mc [186] |
HallP 6c 2c |
Point Group6mm |
Crystal Systemhexagonal |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 106.8 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 148.0 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 225.4 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 246.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 35.6 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 130.5 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 197.3 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 296.0 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 225.4 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 249.1 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 246.6 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 154.2 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 296.5 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 320.3 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 225.4 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 118.6 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 166.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 35.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 130.5 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 154.2 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 152.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 83.0 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 296.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 284.7 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 170.9 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 225.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 249.1 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 177.9 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 177.9 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 166.1 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 320.3 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 189.8 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 296.5 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 320.3 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 225.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 249.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 177.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 83.0 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 47.4 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 256.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 47.4 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 345.3 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 130.5 |
TePb (mp-19717) | <1 0 0> | <1 1 0> | 85.4 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 246.6 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 225.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 296.5 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 256.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 83.0 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 142.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
7.33 | 0.00 | -0.00 |
-0.00 | 7.33 | -0.00 |
0.00 | 0.00 | 3.71 |
Dielectric Tensor εij (total) |
||
---|---|---|
16.77 | -0.00 | -0.00 |
-0.00 | 16.73 | 0.00 |
-0.00 | 0.00 | 3.92 |
Polycrystalline dielectric constant
εpoly∞
6.12
|
Polycrystalline dielectric constant
εpoly
12.48
|
Refractive Index n2.47 |
Potentially ferroelectric?False |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaNiWO6 (mvc-14986) | 0.6562 | 0.293 | 4 |
LiSmAlF6 (mp-8315) | 0.5829 | 0.248 | 4 |
LiCaCrF6 (mp-565468) | 0.6854 | 0.000 | 4 |
NaLa6OsI12 (mp-569905) | 0.5823 | 0.000 | 4 |
SrLa6OsI12 (mp-567419) | 0.6807 | 0.000 | 4 |
CdI2 (mp-571579) | 0.0131 | 0.000 | 2 |
CdI2 (mp-570610) | 0.0159 | 0.000 | 2 |
CdI2 (mp-582042) | 0.0133 | 0.000 | 2 |
CdI2 (mp-570492) | 0.0206 | 0.000 | 2 |
CdI2 (mp-570552) | 0.0143 | 0.000 | 2 |
TiNbS4 (mp-34289) | 0.1938 | 0.020 | 3 |
ZrTiSe4 (mp-570062) | 0.2045 | 0.020 | 3 |
Li2UI6 (mp-570813) | 0.0322 | 0.000 | 3 |
Li2UBr6 (mp-675438) | 0.2239 | 0.000 | 3 |
Li2UBr6 (mp-531472) | 0.1532 | 0.000 | 3 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points42 |
U Values-- |
PseudopotentialsVASP PAW: S Sn_d |
Final Energy/Atom-4.4671 eV |
Corrected Energy-29.4564 eV
-29.4564 eV = -26.8026 eV (uncorrected energy) - 2.6538 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)