Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.749 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.87 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 43009 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
C (mp-66) <1 1 1> <0 0 1> 0.000 66.4
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.002 66.4
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.003 180.2
GaSe (mp-1943) <0 0 1> <0 0 1> 0.005 37.9
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.005 66.4
Mg (mp-153) <0 0 1> <0 0 1> 0.007 113.8
InAs (mp-20305) <1 1 1> <0 0 1> 0.011 66.4
WS2 (mp-224) <1 1 1> <0 0 1> 0.013 237.2
Al (mp-134) <1 0 0> <0 0 1> 0.024 180.2
MoSe2 (mp-1634) <1 1 0> <0 0 1> 0.046 265.6
CdSe (mp-2691) <1 1 1> <0 0 1> 0.049 66.4
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.049 113.8
WS2 (mp-224) <0 0 1> <0 0 1> 0.050 113.8
Al (mp-134) <1 1 1> <0 0 1> 0.053 28.5
ZnO (mp-2133) <1 1 0> <0 0 1> 0.055 151.8
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.062 151.8
BN (mp-984) <0 0 1> <0 0 1> 0.075 37.9
GaSb (mp-1156) <1 1 1> <0 0 1> 0.082 66.4
LaF3 (mp-905) <0 0 1> <0 0 1> 0.090 180.2
TePb (mp-19717) <1 0 0> <0 0 1> 0.090 303.6
TbScO3 (mp-31119) <0 0 1> <0 0 1> 0.100 94.9
Ga2O3 (mp-886) <1 0 1> <0 0 1> 0.111 322.5
TiO2 (mp-2657) <1 0 1> <0 0 1> 0.113 256.1
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.115 9.5
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.117 9.5
LaF3 (mp-905) <1 0 0> <1 1 0> 0.118 267.2
WSe2 (mp-1821) <1 0 1> <0 0 1> 0.118 256.1
Al2O3 (mp-1143) <1 0 0> <1 0 1> 0.123 317.8
LiGaO2 (mp-5854) <0 1 0> <1 0 1> 0.127 198.6
LiF (mp-1138) <1 0 0> <1 1 0> 0.129 66.8
CdS (mp-672) <1 0 1> <1 0 1> 0.129 357.5
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.129 28.5
PbSe (mp-2201) <1 1 1> <0 0 1> 0.135 66.4
Ge3(BiO3)4 (mp-23560) <1 1 1> <0 0 1> 0.136 199.2
GdScO3 (mp-5690) <0 0 1> <0 0 1> 0.143 94.9
TiO2 (mp-2657) <1 1 1> <0 0 1> 0.154 265.6
MgF2 (mp-1249) <1 1 1> <0 0 1> 0.155 151.8
ZnO (mp-2133) <0 0 1> <0 0 1> 0.160 9.5
MgAl2O4 (mp-3536) <1 0 0> <1 0 0> 0.161 270.0
Ge (mp-32) <1 0 0> <1 1 0> 0.166 66.8
YVO4 (mp-19133) <1 0 1> <0 0 1> 0.171 208.7
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.175 180.2
DyScO3 (mp-31120) <0 0 1> <0 0 1> 0.183 94.9
Ni (mp-23) <1 0 0> <0 0 1> 0.195 199.2
LiGaO2 (mp-5854) <1 0 1> <0 0 1> 0.201 313.0
TiO2 (mp-2657) <1 1 0> <0 0 1> 0.207 237.2
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.208 66.4
CdWO4 (mp-19387) <1 0 0> <0 0 1> 0.209 123.3
SiC (mp-8062) <1 1 0> <0 0 1> 0.225 189.7
BN (mp-984) <1 0 0> <0 0 1> 0.228 313.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
368 117 165 0 0 0
117 368 165 0 0 0
165 165 392 0 0 0
0 0 0 184 0 0
0 0 0 0 184 0
0 0 0 0 0 125
Compliance Tensor Sij (10-12Pa-1)
3.4 -0.6 -1.2 0 0 0
-0.6 3.4 -1.2 0 0 0
-1.2 -1.2 3.6 0 0 0
0 0 0 5.4 0 0
0 0 0 0 5.4 0
0 0 0 0 0 8
Shear Modulus GV
144 GPa
Bulk Modulus KV
225 GPa
Shear Modulus GR
136 GPa
Bulk Modulus KR
223 GPa
Shear Modulus GVRH
140 GPa
Bulk Modulus KVRH
224 GPa
Elastic Anisotropy
0.30
Poisson's Ratio
0.24

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
NaMnO2 (mp-971647) 0.0627 0.108 3
V2PC (mp-8044) 0.0679 0.000 3
Ti2SbP (mp-5244) 0.0427 0.000 3
Ti2CS (mp-3732) 0.0202 0.000 3
Hf2CS (mp-13137) 0.0561 0.000 3
Na3Mn2SbO6 (mp-985626) 0.5749 0.000 4
Na3Ni2SbO6 (mp-971678) 0.4807 0.000 4
Na2Li(NiO2)3 (mp-773956) 0.5673 0.031 4
Na3Co2SbO6 (mp-561940) 0.5685 0.015 4
Na3Co2SbO6 (mp-19087) 0.5188 0.000 4
MoC (mp-567925) 0.4322 0.214 2
TlS (mp-998912) 0.4163 0.062 2
ZrP (mp-11345) 0.4349 0.000 2
TiS (mp-557762) 0.3878 0.139 2
NbN (mp-15799) 0.4277 0.206 2
Na6MnNi3(SbO6)2 (mp-1094109) 0.5169 0.005 5
Na (mp-999501) 0.4874 0.124 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Nb_pv P C
Final Energy/Atom
-9.4601 eV
Corrected Energy
-75.6806 eV
-75.6806 eV = -75.6806 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 43009
Submitted by
User remarks:
  • Diniobium phosphide carbide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)