Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.203 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.98 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.305 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 175.4 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 263.1 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 162.7 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 179.3 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 175.4 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 179.3 |
GaN (mp-804) | <1 0 0> | <1 1 1> | 184.8 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 134.1 |
KCl (mp-23193) | <1 1 0> | <0 1 1> | 175.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 162.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 226.3 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 168.7 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 226.3 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 226.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 312.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 226.3 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 1> | 168.7 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 226.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 312.9 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 263.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 223.5 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 226.3 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 301.8 |
TePb (mp-19717) | <1 1 0> | <0 1 1> | 175.4 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 312.9 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 263.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 312.9 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 223.5 |
BN (mp-984) | <0 0 1> | <0 0 1> | 268.2 |
BN (mp-984) | <1 0 1> | <0 0 1> | 312.9 |
BN (mp-984) | <1 1 1> | <0 0 1> | 312.9 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 268.2 |
Al (mp-134) | <1 0 0> | <0 0 1> | 312.9 |
Al (mp-134) | <1 1 0> | <0 1 0> | 226.3 |
Al (mp-134) | <1 1 1> | <1 0 1> | 168.7 |
LiGaO2 (mp-5854) | <1 0 1> | <1 1 0> | 179.3 |
CdTe (mp-406) | <1 0 0> | <0 1 0> | 301.8 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 178.8 |
SiC (mp-7631) | <0 0 1> | <0 1 1> | 175.4 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 268.2 |
TiO2 (mp-2657) | <0 0 1> | <0 1 0> | 150.9 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 150.9 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 75.4 |
TiO2 (mp-2657) | <1 1 0> | <0 1 1> | 175.4 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 150.9 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 0> | 162.7 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 1> | 168.7 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 134.1 |
Mg (mp-153) | <1 1 1> | <1 1 0> | 179.3 |
GaP (mp-2490) | <1 0 0> | <1 1 0> | 179.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.73 | 0.00 | 0.00 |
0.00 | 3.71 | 0.00 |
0.00 | 0.00 | 4.47 |
Dielectric Tensor εij (total) |
||
---|---|---|
12.45 | 0.00 | 0.00 |
0.00 | 10.23 | 0.00 |
0.00 | 0.00 | 240.29 |
Polycrystalline dielectric constant
εpoly∞
3.97
|
Polycrystalline dielectric constant
εpoly
87.66
|
Refractive Index n1.99 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
RbPbI3 (mp-23517) | 0.2337 | 0.000 | 3 |
RbSnI3 (mp-29405) | 0.1518 | 0.000 | 3 |
CsPbI3 (mp-540839) | 0.2782 | 0.000 | 3 |
KSnI3 (mp-1097015) | 0.1372 | 0.000 | 3 |
KSnBr3 (mp-1097014) | 0.1128 | 0.000 | 3 |
LaCrS2O (mp-18885) | 0.6842 | 0.023 | 4 |
KTh(SbSe3)2 (mp-568904) | 0.5214 | 0.000 | 4 |
BaLa(BiS3)2 (mp-555699) | 0.5979 | 0.000 | 4 |
BaMgBiF7 (mvc-10353) | 0.7199 | 0.042 | 4 |
La2InCuSe5 (mp-21390) | 0.7471 | 0.006 | 4 |
Run TypeGGA |
Energy Cutoff700 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Rb_sv Sn_d Br |
Final Energy/Atom-3.1834 eV |
Corrected Energy-63.6683 eV
-63.6683 eV = -63.6683 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)