Final Magnetic Moment1.690 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.192 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.129 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.42 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTi3Ga |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaTe (mp-542812) | <0 0 1> | <1 1 0> | 231.9 |
BN (mp-984) | <0 0 1> | <1 1 1> | 71.0 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 284.0 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 1> | 71.0 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 41.0 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 58.0 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 71.0 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 287.0 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 164.0 |
CsI (mp-614603) | <1 1 0> | <1 1 0> | 173.9 |
Al (mp-134) | <1 0 0> | <1 0 0> | 82.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 164.0 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 164.0 |
SiC (mp-8062) | <1 0 0> | <1 0 0> | 328.0 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 231.9 |
MgF2 (mp-1249) | <1 0 0> | <1 0 0> | 246.0 |
ZnO (mp-2133) | <0 0 1> | <1 0 0> | 328.0 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 328.0 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 231.9 |
LiTaO3 (mp-3666) | <0 0 1> | <1 1 1> | 71.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 164.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 82.0 |
CdWO4 (mp-19387) | <1 0 0> | <1 1 1> | 284.0 |
Au (mp-81) | <1 1 1> | <1 1 1> | 213.0 |
CdS (mp-672) | <0 0 1> | <1 1 0> | 231.9 |
YAlO3 (mp-3792) | <0 1 0> | <1 1 0> | 115.9 |
YAlO3 (mp-3792) | <1 0 1> | <1 0 0> | 246.0 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 328.0 |
CaF2 (mp-2741) | <1 1 0> | <1 1 0> | 173.9 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 205.0 |
CaF2 (mp-2741) | <1 1 1> | <1 1 1> | 213.0 |
NaCl (mp-22862) | <1 0 0> | <1 0 0> | 164.0 |
LiAlO2 (mp-3427) | <1 0 0> | <1 0 0> | 164.0 |
Ge (mp-32) | <1 0 0> | <1 0 0> | 164.0 |
CaCO3 (mp-3953) | <0 0 1> | <1 1 1> | 284.0 |
C (mp-66) | <1 0 0> | <1 0 0> | 164.0 |
SrTiO3 (mp-4651) | <1 0 0> | <1 1 0> | 173.9 |
TiO2 (mp-2657) | <1 0 0> | <1 1 0> | 289.9 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 205.0 |
C (mp-66) | <1 1 1> | <1 1 1> | 284.0 |
C (mp-48) | <0 0 1> | <1 0 0> | 205.0 |
GaP (mp-2490) | <1 1 0> | <1 1 0> | 173.9 |
GaP (mp-2490) | <1 1 1> | <1 1 1> | 213.0 |
Mg (mp-153) | <0 0 1> | <1 1 0> | 173.9 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 0> | 173.9 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 213.0 |
NdGaO3 (mp-3196) | <1 0 0> | <1 1 0> | 173.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 0> | 231.9 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 287.0 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 328.0 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
116 | 104 | 104 | 0 | 0 | 0 |
104 | 116 | 104 | 0 | 0 | 0 |
104 | 104 | 116 | 0 | 0 | 0 |
0 | 0 | 0 | 64 | 0 | 0 |
0 | 0 | 0 | 0 | 64 | 0 |
0 | 0 | 0 | 0 | 0 | 64 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
56.5 | -26.7 | -26.7 | 0 | 0 | 0 |
-26.7 | 56.5 | -26.7 | 0 | 0 | 0 |
-26.7 | -26.7 | 56.5 | 0 | 0 | 0 |
0 | 0 | 0 | 15.6 | 0 | 0 |
0 | 0 | 0 | 0 | 15.6 | 0 |
0 | 0 | 0 | 0 | 0 | 15.6 |
Shear Modulus GV41 GPa |
Bulk Modulus KV108 GPa |
Shear Modulus GR13 GPa |
Bulk Modulus KR108 GPa |
Shear Modulus GVRH27 GPa |
Bulk Modulus KVRH108 GPa |
Elastic Anisotropy10.55 |
Poisson's Ratio0.38 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiGeAu2 (mp-861881) | 0.0000 | 0.000 | 3 |
LaMgZn2 (mp-862662) | 0.0000 | 0.000 | 3 |
NbSiTc2 (mp-864672) | 0.0000 | 0.000 | 3 |
LuTaRu2 (mp-866125) | 0.0000 | 0.000 | 3 |
BeSiP2 (mp-1008491) | 0.0000 | 0.933 | 3 |
VFeCoGe (mp-1063914) | 0.0000 | 0.000 | 4 |
TiFeCoSi (mp-998971) | 0.0000 | 0.029 | 4 |
TiFeCoGe (mp-1018012) | 0.0000 | 0.028 | 4 |
VFeCoAs (mp-1066006) | 0.0000 | 0.211 | 4 |
AlVFeCo (mp-1008530) | 0.0000 | 0.029 | 4 |
K3Si (mp-973528) | 0.0000 | 0.333 | 2 |
NaYb3 (mp-980189) | 0.0000 | 0.083 | 2 |
SnTe3 (mp-978885) | 0.0000 | 0.325 | 2 |
NaCd3 (mp-865077) | 0.0000 | 0.000 | 2 |
FeNi3 (mp-1007854) | 0.0000 | 0.367 | 2 |
Cu (mp-998890) | 0.0000 | 0.037 | 1 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
H2 (mp-632250) | 0.0000 | 0.000 | 1 |
Ge (mp-998883) | 0.0000 | 0.340 | 1 |
U (mp-108) | 0.0000 | 0.271 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ti_pv Ga_d |
Final Energy/Atom-6.8707 eV |
Corrected Energy-27.4829 eV
-27.4829 eV = -27.4829 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)