Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.645 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.065 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.65 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTbH3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 327.9 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 243.4 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 191.3 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 344.3 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 114.8 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 327.9 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 306.0 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 306.0 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 297.5 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 306.0 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 306.0 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 216.4 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 114.8 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 243.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 135.2 |
BaF2 (mp-1029) | <1 0 0> | <1 1 1> | 234.2 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 187.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 243.4 |
InAs (mp-20305) | <1 0 0> | <1 1 1> | 234.2 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 114.8 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 114.8 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 153.0 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 46.8 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 267.8 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 191.3 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 153.0 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 344.3 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 114.8 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 187.4 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 135.2 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 135.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 135.2 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 187.4 |
Te2W (mp-22693) | <0 0 1> | <1 1 1> | 327.9 |
Te2W (mp-22693) | <1 1 0> | <1 1 0> | 114.8 |
Te2W (mp-22693) | <1 1 1> | <1 1 1> | 234.2 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 54.1 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 191.3 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 216.4 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 324.6 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 216.4 |
Te2Mo (mp-602) | <0 0 1> | <1 1 1> | 140.5 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 135.2 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 76.5 |
BN (mp-984) | <1 1 0> | <1 1 0> | 191.3 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 189.3 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 0> | 216.4 |
Ag (mp-124) | <1 1 1> | <1 1 0> | 153.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 297.5 |
MoS2 (mp-1434) | <0 0 1> | <1 1 1> | 140.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Yb2ZnRh (mp-977423) | 0.0000 | 0.000 | 3 |
BaHfMg2 (mp-631500) | 0.0000 | 0.633 | 3 |
CaRe2Si (mp-631420) | 0.0000 | 1.078 | 3 |
PmMgHg2 (mp-862938) | 0.0000 | 0.000 | 3 |
Ac2ZnGa (mp-865535) | 0.0000 | 0.000 | 3 |
VFeCoGe (mp-1063914) | 0.0000 | 0.000 | 4 |
TiFeCoSi (mp-998971) | 0.0000 | 0.029 | 4 |
TiFeCoGe (mp-1018012) | 0.0000 | 0.028 | 4 |
VFeCoAs (mp-1066006) | 0.0000 | 0.211 | 4 |
VGaFeCo (mp-1066581) | 0.0000 | 0.029 | 4 |
Rb3Pb (mp-974832) | 0.0000 | 0.116 | 2 |
RbSr3 (mp-975219) | 0.0000 | 0.143 | 2 |
RbTl3 (mp-975198) | 0.0000 | 0.071 | 2 |
NaCd3 (mp-865077) | 0.0000 | 0.000 | 2 |
Rb3Al (mp-975052) | 0.0000 | 0.365 | 2 |
Cu (mp-998890) | 0.0000 | 0.037 | 1 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
H2 (mp-632250) | 0.0000 | 0.000 | 1 |
Ge (mp-998883) | 0.0000 | 0.340 | 1 |
U (mp-108) | 0.0000 | 0.271 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tb_3 H |
Final Energy/Atom-4.2329 eV |
Corrected Energy-16.9316 eV
-16.9316 eV = -16.9316 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)