Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom1.014 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom1.014 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density10.03 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToPd + N2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 291.8 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 109.4 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 309.5 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 206.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 291.8 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 328.3 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 182.4 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 145.9 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 315.9 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 255.4 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 328.3 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 51.6 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 63.2 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 189.6 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 257.9 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 206.4 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 291.8 |
YVO4 (mp-19133) | <0 0 1> | <1 1 1> | 315.9 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 145.9 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 63.2 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 218.9 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 309.5 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 109.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 328.3 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 36.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 291.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 145.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 206.4 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 182.4 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 145.9 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 252.7 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 257.9 |
YVO4 (mp-19133) | <1 0 0> | <1 1 1> | 189.6 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 182.4 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 109.4 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 182.4 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 182.4 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 291.8 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 255.4 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 182.4 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 291.8 |
BN (mp-984) | <0 0 1> | <1 0 0> | 109.4 |
BN (mp-984) | <1 0 1> | <1 0 0> | 218.9 |
BN (mp-984) | <1 1 0> | <1 1 0> | 257.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 182.4 |
Bi2Se3 (mp-541837) | <1 0 0> | <1 0 0> | 255.4 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 182.4 |
Al (mp-134) | <1 0 0> | <1 0 0> | 145.9 |
Al (mp-134) | <1 1 0> | <1 1 0> | 206.4 |
Al (mp-134) | <1 1 1> | <1 1 1> | 252.7 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
234 | 193 | 193 | 0 | 0 | 0 |
193 | 234 | 193 | 0 | 0 | 0 |
193 | 193 | 234 | 0 | 0 | 0 |
0 | 0 | 0 | -58 | 0 | 0 |
0 | 0 | 0 | 0 | -58 | 0 |
0 | 0 | 0 | 0 | 0 | -58 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
16.7 | -7.5 | -7.5 | 0 | 0 | 0 |
-7.5 | 16.7 | -7.5 | 0 | 0 | 0 |
-7.5 | -7.5 | 16.7 | 0 | 0 | 0 |
0 | 0 | 0 | -17.3 | 0 | 0 |
0 | 0 | 0 | 0 | -17.3 | 0 |
0 | 0 | 0 | 0 | 0 | -17.3 |
Shear Modulus GV-26 GPa |
Bulk Modulus KV207 GPa |
Shear Modulus GR112 GPa |
Bulk Modulus KR207 GPa |
Shear Modulus GVRH43 GPa |
Bulk Modulus KVRH207 GPa |
Elastic Anisotropy-6.18 |
Poisson's Ratio0.40 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiBBr2 (mp-631545) | 0.0000 | 1.679 | 3 |
KHg2B (mp-631525) | 0.0000 | 1.113 | 3 |
BeFe2Si (mp-862669) | 0.0000 | 0.000 | 3 |
PrDyMg2 (mp-862757) | 0.0000 | 0.000 | 3 |
Y2MgRu (mp-865433) | 0.0000 | 0.044 | 3 |
TiFeCoSb (mp-998973) | 0.0000 | 0.186 | 4 |
TiAlFeCo (mp-998980) | 0.0000 | 0.000 | 4 |
TiFeCoGe (mp-1018012) | 0.0000 | 0.028 | 4 |
VFeCoSi (mp-1066609) | 0.0000 | 0.002 | 4 |
VFeCoSb (mp-1066862) | 0.0000 | 0.164 | 4 |
Sn3B (mp-978917) | 0.0000 | 0.939 | 2 |
Rb3Nd (mp-974850) | 0.0000 | 0.619 | 2 |
Mn3Sn (mp-1018023) | 0.0000 | 0.219 | 2 |
Ti3Si (mp-998986) | 0.0000 | 0.194 | 2 |
NbCr3 (mp-999390) | 0.0000 | 0.120 | 2 |
Cu (mp-998890) | 0.0000 | 0.037 | 1 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
H2 (mp-632250) | 0.0000 | 0.000 | 1 |
Ge (mp-998883) | 0.0000 | 0.340 | 1 |
U (mp-108) | 0.0000 | 0.271 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pd N |
Final Energy/Atom-4.8563 eV |
Corrected Energy-19.4252 eV
-19.4252 eV = -19.4252 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)