Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.108 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.210 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.46 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNbNi + Nb |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 339.5 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 254.1 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 113.2 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 254.1 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 161.7 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 294.0 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 277.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 147.0 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 254.1 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 198.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 32.7 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 46.2 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 277.2 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 81.7 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 198.0 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 115.5 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 81.7 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 254.1 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 92.4 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 245.0 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 84.9 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 369.6 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 141.5 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 207.9 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 81.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 1> | 56.6 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 65.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 92.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 130.7 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 277.2 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 46.2 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 147.0 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 207.9 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 198.0 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 46.2 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 277.2 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 28.3 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 32.7 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 16.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 23.1 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 245.0 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 277.2 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 294.0 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 184.8 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 198.0 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 207.9 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 161.7 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 207.9 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 212.3 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 16.3 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
133 | 275 | 275 | 0 | 0 | 0 |
275 | 133 | 275 | 0 | 0 | 0 |
275 | 275 | 133 | 0 | 0 | 0 |
0 | 0 | 0 | 11 | 0 | 0 |
0 | 0 | 0 | 0 | 11 | 0 |
0 | 0 | 0 | 0 | 0 | 11 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
-4.2 | 2.8 | 2.8 | 0 | 0 | 0 |
2.8 | -4.2 | 2.8 | 0 | 0 | 0 |
2.8 | 2.8 | -4.2 | 0 | 0 | 0 |
0 | 0 | 0 | 93.4 | 0 | 0 |
0 | 0 | 0 | 0 | 93.4 | 0 |
0 | 0 | 0 | 0 | 0 | 93.4 |
Shear Modulus GV-22 GPa |
Bulk Modulus KV228 GPa |
Shear Modulus GR20 GPa |
Bulk Modulus KR228 GPa |
Shear Modulus GVRH-1 GPa |
Bulk Modulus KVRH228 GPa |
Elastic Anisotropy-10.53 |
Poisson's Ratio0.50 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnCu2Ni (mp-30593) | 0.1125 | 0.005 | 3 |
CrCoPt2 (mp-570863) | 0.0492 | 0.000 | 3 |
LiCa6Ge (mp-12609) | 0.0000 | 0.180 | 3 |
GaFeNi2 (mp-1065359) | 0.0412 | 0.066 | 3 |
GaCo2Ni (mp-1018060) | 0.0157 | 0.075 | 3 |
Cr8Ni50Mo15W2 (mp-767372) | 0.2155 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.3608 | 0.118 | 4 |
CrFeCoNi (mp-1096923) | 0.4019 | 0.193 | 4 |
BeNi3 (mp-984717) | 0.0000 | 0.076 | 2 |
NaN3 (mp-1064161) | 0.0000 | 2.843 | 2 |
EuPd3 (mp-636279) | 0.0000 | 0.001 | 2 |
TbTl3 (mp-1886) | 0.0000 | 0.000 | 2 |
HoSn3 (mp-11477) | 0.0000 | 0.025 | 2 |
Na (mp-974558) | 0.0000 | 0.001 | 1 |
Br (mp-998870) | 0.0000 | 0.666 | 1 |
Mn (mp-8634) | 0.0000 | 0.083 | 1 |
Pb (mp-20483) | 0.0000 | 0.000 | 1 |
Cu (mp-30) | 0.0000 | 0.000 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nb_pv Ni_pv |
Final Energy/Atom-8.9128 eV |
Corrected Energy-35.6511 eV
-35.6511 eV = -35.6511 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)