Material Details

Final Magnetic Moment
0.192 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-0.356 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.25 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63mc [186]
Hall
P 6c 2c
Point Group
6mm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 643594 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ge(Bi3O5)4 (mp-23352) <1 1 1> <0 0 1> 0.000 183.7
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.000 199.0
C (mp-66) <1 1 1> <0 0 1> 0.000 199.0
CdS (mp-672) <0 0 1> <0 0 1> 0.000 15.3
CdS (mp-672) <1 0 1> <1 0 1> 0.000 32.6
CdS (mp-672) <1 1 1> <1 1 1> 0.000 52.1
CdS (mp-672) <1 1 0> <1 1 0> 0.000 49.8
CdS (mp-672) <1 0 0> <1 0 0> 0.000 28.8
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.001 199.0
CsI (mp-614603) <1 1 1> <0 0 1> 0.001 107.2
AlN (mp-661) <1 0 0> <1 0 0> 0.002 172.5
InAs (mp-20305) <1 1 1> <0 0 1> 0.003 199.0
SiC (mp-8062) <1 1 0> <1 1 0> 0.003 298.8
CeO2 (mp-20194) <1 0 0> <1 0 1> 0.004 358.3
Si (mp-149) <1 0 0> <1 0 1> 0.004 358.3
ZrO2 (mp-2858) <1 0 -1> <1 0 0> 0.005 143.8
Mg (mp-153) <0 0 1> <0 0 1> 0.006 61.2
InP (mp-20351) <1 1 1> <0 0 1> 0.006 61.2
GdScO3 (mp-5690) <0 0 1> <1 0 0> 0.011 287.6
SrTiO3 (mp-4651) <1 0 1> <0 0 1> 0.012 107.2
SiC (mp-11714) <0 0 1> <0 0 1> 0.015 107.2
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.018 15.3
SiC (mp-7631) <0 0 1> <0 0 1> 0.019 107.2
NaCl (mp-22862) <1 1 0> <1 0 1> 0.024 228.0
ZrO2 (mp-2858) <1 0 0> <0 0 1> 0.026 229.6
LiTaO3 (mp-3666) <1 0 1> <1 0 1> 0.026 228.0
LaAlO3 (mp-2920) <1 0 0> <1 0 0> 0.027 143.8
CdSe (mp-2691) <1 1 1> <0 0 1> 0.029 199.0
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.029 61.2
WS2 (mp-224) <0 0 1> <0 0 1> 0.029 61.2
BN (mp-984) <1 0 1> <1 0 1> 0.032 260.6
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.035 183.7
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.035 183.7
GaN (mp-804) <1 0 1> <1 0 1> 0.036 228.0
AlN (mp-661) <1 1 1> <0 0 1> 0.036 229.6
Te2W (mp-22693) <1 1 1> <0 0 1> 0.038 229.6
TiO2 (mp-2657) <1 1 1> <0 0 1> 0.038 290.9
BaTiO3 (mp-5986) <0 0 1> <1 1 1> 0.038 208.4
YVO4 (mp-19133) <1 0 1> <1 1 1> 0.038 208.4
Te2W (mp-22693) <0 1 1> <1 0 1> 0.039 293.2
YVO4 (mp-19133) <1 1 0> <1 0 0> 0.039 258.8
Al2O3 (mp-1143) <1 0 1> <1 1 0> 0.041 199.2
Ga2O3 (mp-886) <1 1 0> <0 0 1> 0.043 290.9
DyScO3 (mp-31120) <0 1 0> <1 1 1> 0.044 260.5
Ag (mp-124) <1 1 0> <0 0 1> 0.045 122.5
GaSb (mp-1156) <1 1 1> <0 0 1> 0.045 199.0
Al (mp-134) <1 1 0> <1 0 1> 0.046 162.9
LaF3 (mp-905) <0 0 1> <0 0 1> 0.046 45.9
Cu (mp-30) <1 0 0> <1 1 1> 0.046 52.1
TiO2 (mp-2657) <1 0 0> <0 0 1> 0.047 137.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
71 45 40 0 0 0
45 71 40 0 0 0
40 40 71 0 0 0
0 0 0 12 0 0
0 0 0 0 12 0
0 0 0 0 0 13
Compliance Tensor Sij (10-12Pa-1)
26.3 -12.2 -8 0 0 0
-12.2 26.3 -8 0 0 0
-8 -8 23.1 0 0 0
0 0 0 80.6 0 0
0 0 0 0 80.6 0
0 0 0 0 0 77
Shear Modulus GV
13 GPa
Bulk Modulus KV
51 GPa
Shear Modulus GR
13 GPa
Bulk Modulus KR
51 GPa
Shear Modulus GVRH
13 GPa
Bulk Modulus KVRH
51 GPa
Elastic Anisotropy
0.05
Poisson's Ratio
0.38

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
BeSiN2 (mp-7913) 0.0592 0.000 3
LiInSe2 (mp-20310) 0.0995 0.001 3
MgSnN2 (mp-1029791) 0.1540 0.000 3
ZnSnN2 (mp-1029469) 0.0631 0.000 3
Zn2SbN3 (mp-1029334) 0.1427 0.004 3
Li2ZnSnS4 (mp-555186) 0.1888 0.000 4
ZnGaNO (mp-558481) 0.2849 0.058 4
ZnCu2GeS4 (mp-6408) 0.3055 0.000 4
CoCu2SiS4 (mp-11769) 0.3083 0.065 4
ZnCu2SnS4 (mp-1079541) 0.3105 0.000 4
SiC (mp-7140) 0.0204 0.004 2
GaSb (mp-1018059) 0.0196 0.013 2
AlSb (mp-1018100) 0.0054 0.008 2
TlN (mp-1017982) 0.0171 0.721 2
InAs (mp-1007652) 0.0066 0.006 2
Ge (mp-1007760) 0.0321 0.121 1
Si (mp-165) 0.0401 0.011 1
C (mp-611426) 0.2274 0.146 1
C (mp-47) 0.0448 0.162 1
Ge (mp-1091415) 0.2401 0.008 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mn_pv Se
Final Energy/Atom
-6.6862 eV
Corrected Energy
-27.6887 eV
Uncorrected energy = -26.7447 eV Composition-based energy adjustment (-0.472 eV/atom x 2.0 atoms) = -0.9440 eV Corrected energy = -27.6887 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 643594
Submitted by
User remarks:
  • Manganese selenide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)