Final Magnetic Moment4.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.539 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.049 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.69 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToV2ZnO4 + Zn3(PO4)2 + VPO4 |
Band Gap1.650 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 278.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 325.2 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 271.3 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 203.3 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 325.2 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 139.3 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 101.7 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 231.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 325.2 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 139.3 |
BaF2 (mp-1029) | <1 0 0> | <0 1 1> | 203.3 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 101.7 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 232.3 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 325.2 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 232.3 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 271.3 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 211.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 139.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 325.2 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 105.9 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 90.4 |
Te2W (mp-22693) | <1 0 1> | <0 1 1> | 101.7 |
Te2W (mp-22693) | <1 1 0> | <1 0 1> | 115.7 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 105.9 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 46.5 |
YVO4 (mp-19133) | <1 0 1> | <1 1 0> | 139.3 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 325.2 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 211.8 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 232.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 271.3 |
GaSe (mp-1943) | <1 0 0> | <0 1 0> | 271.3 |
BN (mp-984) | <0 0 1> | <0 0 1> | 325.2 |
BN (mp-984) | <1 0 0> | <1 0 1> | 115.7 |
BN (mp-984) | <1 1 0> | <0 1 0> | 271.3 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 139.4 |
MoS2 (mp-1434) | <1 0 0> | <0 1 0> | 271.3 |
MoS2 (mp-1434) | <1 0 1> | <0 1 0> | 271.3 |
Al (mp-134) | <1 0 0> | <1 0 0> | 211.8 |
Al (mp-134) | <1 1 0> | <1 1 0> | 139.3 |
Al (mp-134) | <1 1 1> | <0 0 1> | 325.2 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 325.2 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 325.2 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 139.4 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 46.5 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 232.3 |
SiC (mp-7631) | <1 0 0> | <1 0 1> | 231.3 |
SiC (mp-7631) | <1 1 0> | <1 0 1> | 231.3 |
MgO (mp-1265) | <1 1 0> | <1 0 1> | 231.3 |
C (mp-66) | <1 1 0> | <0 0 1> | 325.2 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 325.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CrPO4 (mp-850489) | 0.6933 | 0.067 | 3 |
Mn2PO5 (mp-770538) | 0.6363 | 0.011 | 3 |
Zn3(PO4)2 (mp-31005) | 0.6457 | 0.019 | 3 |
Cr5(PO4)4 (mp-540446) | 0.5711 | 0.007 | 3 |
Cr5(PO4)4 (mp-775246) | 0.5857 | 0.007 | 3 |
MgFe2P2O9 (mvc-10158) | 0.2218 | 0.043 | 4 |
MgTi2P2O9 (mvc-9760) | 0.2502 | 0.144 | 4 |
Mn2ZnP2O9 (mvc-10149) | 0.2968 | 0.076 | 4 |
MgCr2P2O9 (mvc-10041) | 0.2786 | 0.751 | 4 |
ZnCr2P2O9 (mvc-10043) | 0.2382 | 0.200 | 4 |
MgMnNiP2O9 (mvc-8274) | 0.4056 | 0.242 | 5 |
MgFeNiP2O9 (mvc-8280) | 0.3415 | 0.087 | 5 |
MgCoNiP2O9 (mvc-8295) | 0.3415 | 0.102 | 5 |
ZnFeNiP2O9 (mvc-8277) | 0.3379 | 0.272 | 5 |
MnZnNiP2O9 (mvc-8316) | 0.3836 | 0.064 | 5 |
Li4TiNi3Sn2(PO4)6 (mp-778249) | 0.5299 | 0.173 | 6 |
LiMnVP2(HO5)2 (mp-765074) | 0.5704 | 0.045 | 6 |
LiMnVP2(HO5)2 (mp-766999) | 0.5672 | 0.039 | 6 |
LiMnVP2(HO5)2 (mp-765151) | 0.5692 | 0.154 | 6 |
LiMnVP2(HO5)2 (mp-765107) | 0.5472 | 0.086 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: V_pv Zn P O |
Final Energy/Atom-7.1886 eV |
Corrected Energy-441.3022 eV
-441.3022 eV = -402.5637 eV (uncorrected energy) - 25.2824 eV (MP Anion Correction) - 13.4560 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)