Final Magnetic Moment2.999 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.235 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.218 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.52 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToZn(CuO2)2 + MnO2 |
Band Gap0.054 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 211.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 158.8 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 302.8 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 277.1 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 264.7 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 158.8 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 227.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 264.7 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 75.7 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 211.8 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 227.1 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 227.1 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 264.7 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 97.7 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 317.7 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 302.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 264.7 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 264.7 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 158.8 |
Te2W (mp-22693) | <1 0 0> | <0 1 0> | 302.8 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 92.4 |
YVO4 (mp-19133) | <1 0 1> | <0 1 1> | 277.1 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 264.7 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 0> | 151.4 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 211.8 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 317.7 |
NdGaO3 (mp-3196) | <1 1 1> | <0 1 1> | 277.1 |
Ga2O3 (mp-886) | <0 1 0> | <1 0 0> | 293.2 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 293.2 |
Ga2O3 (mp-886) | <1 1 0> | <1 0 0> | 293.2 |
Au (mp-81) | <1 1 0> | <1 0 0> | 97.7 |
Au (mp-81) | <1 1 1> | <0 0 1> | 211.8 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 158.8 |
CdSe (mp-2691) | <1 1 0> | <0 1 0> | 227.1 |
WS2 (mp-224) | <1 0 0> | <0 1 1> | 92.4 |
C (mp-48) | <0 0 1> | <1 1 0> | 247.2 |
C (mp-48) | <1 0 0> | <0 0 1> | 211.8 |
C (mp-48) | <1 1 0> | <0 1 0> | 302.8 |
C (mp-48) | <1 1 1> | <0 1 0> | 302.8 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 264.7 |
ZrO2 (mp-2858) | <0 1 0> | <0 0 1> | 317.7 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 264.7 |
ZrO2 (mp-2858) | <1 0 1> | <0 0 1> | 211.8 |
YAlO3 (mp-3792) | <1 1 1> | <0 0 1> | 317.7 |
SiC (mp-8062) | <1 1 0> | <1 0 0> | 293.2 |
CdWO4 (mp-19387) | <0 0 1> | <1 1 0> | 123.6 |
CdWO4 (mp-19387) | <1 0 0> | <1 1 0> | 123.6 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 293.2 |
MgF2 (mp-1249) | <1 0 0> | <1 1 0> | 247.2 |
MgF2 (mp-1249) | <1 1 0> | <0 1 0> | 302.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn2Si2O7 (mp-767344) | 0.6137 | 0.089 | 3 |
Mn2PO5 (mp-770532) | 0.5995 | 0.039 | 3 |
Co3(AsO4)2 (mp-25740) | 0.5418 | 0.003 | 3 |
Ni(GeO3)2 (mvc-8467) | 0.5745 | 0.230 | 3 |
Zn2As2O7 (mp-781624) | 0.5598 | 0.013 | 3 |
MgV2(CuO4)2 (mvc-12094) | 0.2643 | 0.014 | 4 |
MgMn2(CuO4)2 (mvc-10463) | 0.1370 | 0.205 | 4 |
MgCu2(NiO4)2 (mvc-10476) | 0.2725 | 0.251 | 4 |
ZnCr2(CuO4)2 (mvc-10466) | 0.2603 | 0.110 | 4 |
MgCu2(MoO4)2 (mvc-10462) | 0.2686 | 0.067 | 4 |
LiCrPO4F (mp-762791) | 0.7444 | 0.072 | 5 |
Li7MnP4O14F (mp-762708) | 0.6713 | 0.068 | 5 |
Li7FeP4O14F (mp-762690) | 0.6398 | 0.066 | 5 |
Al2CuSi2O7F2 (mp-557084) | 0.7250 | 0.016 | 5 |
Li7CuAs4ClO14 (mp-769204) | 0.6972 | 0.074 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Mn_pv Zn Cu_pv O |
Final Energy/Atom-5.7266 eV |
Corrected Energy-333.7025 eV
-333.7025 eV = -297.7824 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction) - 13.4468 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)