Final Magnetic Moment0.065 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.280 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.262 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.97 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCa(CuO2)2 + CoO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 231.4 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 289.2 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 289.2 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 237.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 173.5 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 244.9 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 104.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 209.0 |
CdS (mp-672) | <0 0 1> | <1 1 0> | 262.1 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 316.4 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 209.0 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 237.3 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 173.5 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 231.4 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 316.4 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 173.5 |
GaSe (mp-1943) | <1 1 0> | <0 0 1> | 115.7 |
BN (mp-984) | <0 0 1> | <0 0 1> | 173.5 |
Al (mp-134) | <1 1 0> | <1 0 0> | 209.0 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 231.4 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 289.2 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 289.2 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 173.5 |
TeO2 (mp-2125) | <1 0 0> | <1 0 0> | 209.0 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 231.4 |
Fe3O4 (mp-19306) | <1 1 0> | <1 0 0> | 104.5 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 289.2 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 104.5 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 173.5 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 209.0 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 57.8 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 57.8 |
C (mp-66) | <1 1 1> | <0 0 1> | 173.5 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 289.2 |
PbS (mp-21276) | <1 1 0> | <1 0 0> | 104.5 |
InP (mp-20351) | <1 0 0> | <0 1 0> | 316.4 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 104.5 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 173.5 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 173.5 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 0> | 209.0 |
SiC (mp-11714) | <1 0 1> | <0 0 1> | 231.4 |
MoSe2 (mp-1634) | <0 0 1> | <0 1 0> | 316.4 |
Ga2O3 (mp-886) | <0 1 0> | <1 0 0> | 209.0 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 0> | 237.3 |
Au (mp-81) | <1 1 0> | <0 1 0> | 316.4 |
WS2 (mp-224) | <1 0 0> | <0 1 0> | 316.4 |
C (mp-48) | <0 0 1> | <0 1 1> | 196.0 |
WSe2 (mp-1821) | <0 0 1> | <0 1 0> | 316.4 |
NaCl (mp-22862) | <1 1 0> | <0 1 0> | 316.4 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 289.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
VCuO4 (mvc-12122) | 0.6701 | 0.123 | 3 |
Cr5(Si2O7)2 (mp-767345) | 0.6551 | 0.100 | 3 |
Zn4As2O9 (mp-555797) | 0.5752 | 0.008 | 3 |
Mg(SbO2)2 (mvc-9831) | 0.6457 | 0.218 | 3 |
V2Zn4O9 (mp-504923) | 0.6670 | 0.019 | 3 |
ZnCuW2O7 (mvc-6749) | 0.5794 | 0.261 | 4 |
MgCo2(PO4)2 (mvc-10188) | 0.5939 | 0.286 | 4 |
MgNi2(PO4)2 (mvc-10192) | 0.4967 | 0.109 | 4 |
CaV2(CuO4)2 (mvc-10482) | 0.5627 | 0.061 | 4 |
CaFe2(CuO4)2 (mvc-10511) | 0.5145 | 0.475 | 4 |
Mg5Al4Fe(SiO4)6 (mp-743769) | 0.6379 | 0.280 | 5 |
NaMg3Si4O11F (mp-695597) | 0.7422 | 0.281 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Ca_sv Co Cu_pv O |
Final Energy/Atom-5.4059 eV |
Corrected Energy-318.5720 eV
-318.5720 eV = -281.1067 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction) - 14.9920 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)