Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.681 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.126 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.50 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBi4O7 + MgO |
Band Gap0.460 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 180.7 |
AlN (mp-661) | <0 0 1> | <1 0 -1> | 264.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 156.3 |
AlN (mp-661) | <1 0 1> | <1 0 -1> | 308.2 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 108.4 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 108.4 |
GaN (mp-804) | <1 0 0> | <1 0 -1> | 132.1 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 180.7 |
GaN (mp-804) | <1 0 1> | <1 0 -1> | 176.1 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 156.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 260.4 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 312.4 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 325.2 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 260.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 208.3 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 260.4 |
CdS (mp-672) | <1 1 0> | <1 0 -1> | 264.1 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 361.3 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 289.1 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 88.0 |
CdS (mp-672) | <1 1 1> | <1 0 -1> | 308.2 |
LiF (mp-1138) | <1 1 0> | <1 0 -1> | 264.1 |
LiF (mp-1138) | <1 1 1> | <1 0 1> | 234.3 |
Te2W (mp-22693) | <0 0 1> | <1 0 -1> | 44.0 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 52.1 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 216.8 |
Te2W (mp-22693) | <0 1 1> | <1 0 -1> | 176.1 |
YVO4 (mp-19133) | <1 1 0> | <1 0 -1> | 132.1 |
Ag (mp-124) | <1 1 0> | <1 0 -1> | 264.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 -1> | 352.2 |
BN (mp-984) | <1 0 0> | <0 0 1> | 156.3 |
BN (mp-984) | <1 1 0> | <0 0 1> | 260.4 |
BN (mp-984) | <1 1 1> | <0 0 1> | 260.4 |
GaSe (mp-1943) | <0 0 1> | <1 0 1> | 312.4 |
BN (mp-984) | <0 0 1> | <0 0 1> | 260.4 |
BN (mp-984) | <1 0 1> | <1 0 0> | 216.8 |
LiNbO3 (mp-3731) | <1 1 0> | <0 0 1> | 260.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 289.1 |
LiNbO3 (mp-3731) | <1 0 1> | <1 0 0> | 325.2 |
Al (mp-134) | <1 1 1> | <1 0 0> | 361.3 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 260.4 |
Al (mp-134) | <1 1 0> | <0 0 1> | 208.3 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 -1> | 220.1 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 208.3 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 -1> | 132.1 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 180.7 |
MgO (mp-1265) | <1 0 0> | <1 0 -1> | 220.1 |
MgO (mp-1265) | <1 1 1> | <1 0 0> | 252.9 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 252.9 |
C (mp-66) | <1 0 0> | <1 0 0> | 289.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Al2(BiO3)3 (mvc-12722) | 0.6351 | 0.124 | 3 |
CrOF (mp-764359) | 0.6025 | 0.098 | 3 |
Na4Ti7O16 (mp-761140) | 0.6896 | 0.091 | 3 |
Li2Mn2F7 (mp-763794) | 0.6656 | 0.054 | 3 |
Ba2Sr7I18 (mp-752682) | 0.5922 | 0.054 | 3 |
Li4Mn3OF11 (mp-766928) | 0.6571 | 0.073 | 4 |
MgCuBiO5 (mvc-7427) | 0.7249 | 0.113 | 4 |
MgCoBi2O7 (mvc-7725) | 0.7125 | 0.198 | 4 |
ZnCoBi2O7 (mvc-7720) | 0.6946 | 0.168 | 4 |
Li3V4(OF3)3 (mp-766144) | 0.7199 | 0.071 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv Bi O |
Final Energy/Atom-5.6141 eV |
Corrected Energy-78.6021 eV
-78.6021 eV = -72.9837 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)