Final Magnetic Moment0.197 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.835 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.317 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.74 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCa2Mn3O8 + Ca(NiO2)2 + CaO + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2 [5] |
HallC 2y |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 246.4 |
LaAlO3 (mp-2920) | <1 1 1> | <0 0 1> | 246.4 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 234.6 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 105.9 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 331.4 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 117.3 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 164.3 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 276.2 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 331.4 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 331.4 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 165.7 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 331.4 |
GaN (mp-804) | <1 1 0> | <1 0 -1> | 287.0 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 220.9 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 331.4 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 234.6 |
SiO2 (mp-6930) | <1 0 1> | <1 0 -1> | 287.0 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 241.7 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 82.1 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 58.7 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 176.0 |
KCl (mp-23193) | <1 1 1> | <1 0 -1> | 287.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 -1> | 220.9 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 117.3 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 164.3 |
TePb (mp-19717) | <1 1 1> | <1 0 0> | 293.3 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 246.4 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 293.3 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 234.6 |
YVO4 (mp-19133) | <1 1 0> | <1 0 -1> | 191.3 |
BN (mp-984) | <0 0 1> | <1 0 0> | 293.3 |
BN (mp-984) | <1 1 0> | <0 1 0> | 165.7 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 176.0 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 246.4 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 176.0 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 293.3 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 176.0 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 -1> | 95.7 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 293.3 |
BN (mp-984) | <1 0 1> | <0 1 0> | 220.9 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 -1> | 287.0 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 246.4 |
LiNbO3 (mp-3731) | <1 1 0> | <0 0 1> | 246.4 |
LiNbO3 (mp-3731) | <1 1 1> | <0 0 1> | 246.4 |
MoS2 (mp-1434) | <0 0 1> | <1 0 1> | 105.9 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 165.7 |
SiC (mp-7631) | <1 0 1> | <1 0 0> | 234.6 |
LiTaO3 (mp-3666) | <1 1 0> | <0 0 1> | 246.4 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 176.0 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 234.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
KMn2O4 (mp-1003314) | 0.5635 | 0.000 | 3 |
KMn2O4 (mp-763541) | 0.5728 | 0.001 | 3 |
Li4TbF8 (mp-505089) | 0.5118 | 0.011 | 3 |
Sr4Cr3O9 (mp-566516) | 0.5660 | 0.158 | 3 |
Ca(Sn2O3)2 (mvc-404) | 0.5391 | 0.307 | 3 |
Ca2CoRhO6 (mvc-13129) | 0.4639 | 0.209 | 4 |
Ca5Sc2(CoO6)2 (mvc-13126) | 0.6373 | 0.013 | 4 |
Ca5Mn2(NiO6)2 (mvc-13112) | 0.4512 | 0.106 | 4 |
Ca2FeRhO6 (mvc-14247) | 0.4521 | 0.298 | 4 |
Li5La3Nb2O12 (mp-774721) | 0.6256 | 0.050 | 4 |
Ca5Gd3Ti5Mn3O24 (mp-744410) | 0.5867 | 0.013 | 5 |
Na3HoTi2Nb2O12 (mp-676988) | 0.6059 | 0.009 | 5 |
Ca5Y3Ti5Mn3O24 (mp-743716) | 0.6029 | 0.156 | 5 |
Ca5Ho3Ti5Mn3O24 (mp-743699) | 0.6091 | 0.159 | 5 |
Ca5Dy3Ti5Mn3O24 (mp-743698) | 0.6027 | 0.018 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVNi: 6.2 eV |
PseudopotentialsVASP PAW: Ca_sv Mn_pv Ni_pv O |
Final Energy/Atom-5.8922 eV |
Corrected Energy-133.9603 eV
-133.9603 eV = -117.8431 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction) - 7.6897 eV (MP Advanced Correction)
|