Final Magnetic Moment7.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.037 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.134 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.91 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCo3O4 + Al2CoO4 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFd3m [227] |
HallF 4d 2 3 1d |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <1 1 0> | 290.2 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 273.6 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 205.2 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 273.6 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 290.2 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 290.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 68.4 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 96.7 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 273.6 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 193.4 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 68.4 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 96.7 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 68.4 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 96.7 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 273.6 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 273.6 |
Al (mp-134) | <1 0 0> | <1 0 0> | 273.6 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 205.2 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 136.8 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 193.4 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 118.5 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 290.2 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 205.2 |
LiTaO3 (mp-3666) | <1 0 0> | <1 1 0> | 290.2 |
MgO (mp-1265) | <1 0 0> | <1 1 0> | 290.2 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 273.6 |
GdScO3 (mp-5690) | <1 1 0> | <1 1 0> | 193.4 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 273.6 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 68.4 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 96.7 |
InSb (mp-20012) | <1 1 0> | <1 1 0> | 193.4 |
NdGaO3 (mp-3196) | <0 0 1> | <1 0 0> | 273.6 |
Ga2O3 (mp-886) | <0 1 0> | <1 1 0> | 290.2 |
Ga2O3 (mp-886) | <1 1 0> | <1 1 0> | 290.2 |
Au (mp-81) | <1 1 0> | <1 1 0> | 96.7 |
ZrO2 (mp-2858) | <1 1 0> | <1 0 0> | 273.6 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 205.2 |
C (mp-66) | <1 1 0> | <1 1 0> | 290.2 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 0> | 136.8 |
GdScO3 (mp-5690) | <1 0 0> | <1 1 0> | 96.7 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 205.2 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 273.6 |
TiO2 (mp-390) | <0 0 1> | <1 1 0> | 290.2 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 193.4 |
MgAl2O4 (mp-3536) | <1 0 0> | <1 0 0> | 68.4 |
MgAl2O4 (mp-3536) | <1 1 0> | <1 1 0> | 96.7 |
SrTiO3 (mp-4651) | <0 0 1> | <1 0 0> | 273.6 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 273.6 |
Ga2O3 (mp-886) | <1 0 0> | <1 1 0> | 290.2 |
Si (mp-149) | <1 0 0> | <1 0 0> | 273.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mg2GeO4 (mp-3904) | 0.0600 | 0.000 | 3 |
In2NiS4 (mp-20960) | 0.0628 | 0.107 | 3 |
Co2GeO4 (mp-18758) | 0.0758 | 0.019 | 3 |
Al(FeO2)2 (mp-541934) | 0.0669 | 0.056 | 3 |
Zn(BiO2)2 (mvc-4703) | 0.0724 | 0.195 | 3 |
LiVNiO4 (mp-771631) | 0.1703 | 0.001 | 4 |
Li7V6Ni5O24 (mp-769574) | 0.2501 | 0.013 | 4 |
LiNbCoO4 (mp-772384) | 0.2169 | 0.030 | 4 |
LiNbFeO4 (mp-772339) | 0.2409 | 0.006 | 4 |
LiVCoO4 (mp-768046) | 0.2038 | 0.005 | 4 |
Fe3O4 (mp-715490) | 0.1345 | 0.089 | 2 |
Fe3O4 (mp-567124) | 0.2026 | 0.015 | 2 |
Fe3O4 (mp-715558) | 0.1882 | 0.076 | 2 |
Fe3O4 (mp-716052) | 0.2044 | 0.073 | 2 |
Fe3O4 (mp-715811) | 0.1922 | 0.076 | 2 |
Li4Ti3Cr3(SnO8)2 (mp-776780) | 0.3850 | 0.029 | 5 |
Li4Ti3Cr3(WO8)2 (mp-773537) | 0.3857 | 0.043 | 5 |
Li4Cr3Fe3(TeO8)2 (mp-773518) | 0.3765 | 0.868 | 5 |
Li4Fe3Ni3(TeO8)2 (mp-773382) | 0.3993 | 0.009 | 5 |
Li4Cr3Fe3(SbO8)2 (mp-771925) | 0.3790 | 0.831 | 5 |
Li3MnFeCo(PO4)3 (mp-764931) | 0.6889 | 0.015 | 6 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.6797 | 0.015 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.6853 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764707) | 0.6922 | 0.035 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.6809 | 0.032 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Al Co O |
Final Energy/Atom-6.4934 eV |
Corrected Energy-104.0217 eV
-104.0217 eV = -90.9074 eV (uncorrected energy) - 7.4960 eV (MP Advanced Correction) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)