Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.425 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.98 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.871 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [166] |
Hall-R 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | elastic energy [meV] | MCIA† [Å2] |
---|---|---|---|---|
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 0.002 | 136.2 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 0.004 | 229.3 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 0.006 | 193.5 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 0.006 | 28.7 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 0.006 | 28.7 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 0.008 | 222.2 |
TbScO3 (mp-31119) | <1 0 0> | <0 0 1> | 0.017 | 229.3 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 0.024 | 50.2 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 0.033 | 28.7 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 0.037 | 351.2 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 0.039 | 351.2 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 0.041 | 222.2 |
MgAl2O4 (mp-3536) | <1 1 1> | <0 0 1> | 0.041 | 114.7 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 0.043 | 21.5 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 0.043 | 93.2 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 0.044 | 245.9 |
Al (mp-134) | <1 0 0> | <0 0 1> | 0.045 | 114.7 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 0.049 | 179.2 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 0.052 | 250.8 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 0.052 | 215.0 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 0.061 | 222.2 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 0.064 | 93.2 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 0.069 | 279.5 |
WSe2 (mp-1821) | <1 1 0> | <0 0 1> | 0.070 | 86.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 0.073 | 114.7 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 0.075 | 215.0 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 0.090 | 229.3 |
SiC (mp-11714) | <1 0 1> | <0 0 1> | 0.094 | 229.3 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 0.098 | 293.8 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 0.098 | 98.4 |
SrTiO3 (mp-4651) | <0 0 1> | <0 0 1> | 0.109 | 250.8 |
NaCl (mp-22862) | <1 0 0> | <1 0 0> | 0.113 | 98.4 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 0.119 | 93.2 |
Al (mp-134) | <1 1 1> | <0 0 1> | 0.120 | 28.7 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 0.128 | 147.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 0.131 | 21.5 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 0.134 | 114.7 |
GaTe (mp-542812) | <1 0 0> | <0 0 1> | 0.138 | 315.3 |
NaCl (mp-22862) | <1 1 0> | <0 0 1> | 0.141 | 229.3 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 0.141 | 98.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 0.144 | 114.7 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 0.145 | 279.5 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 0.154 | 265.2 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 0.155 | 215.0 |
Al (mp-134) | <1 1 0> | <0 0 1> | 0.164 | 114.7 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 0.168 | 193.5 |
BN (mp-984) | <0 0 1> | <0 0 1> | 0.170 | 21.5 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 0.171 | 250.8 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 0.183 | 250.8 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 0.184 | 136.2 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
277 | 68 | 70 | 3 | 0 | 0 |
68 | 277 | 70 | -3 | 0 | 0 |
70 | 70 | 520 | 0 | 0 | 0 |
3 | -3 | 0 | 40 | 0 | 0 |
0 | 0 | 0 | 0 | 40 | 3 |
0 | 0 | 0 | 0 | 3 | 105 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
3.9 | -0.9 | -0.4 | -0.4 | 0 | 0 |
-0.9 | 3.9 | -0.4 | 0.4 | 0 | 0 |
-0.4 | -0.4 | 2 | 0 | 0 | 0 |
-0.4 | 0.4 | 0 | 25.3 | 0 | 0 |
0 | 0 | 0 | 0 | 25.3 | -0.8 |
0 | 0 | 0 | 0 | -0.8 | 9.6 |
Shear Modulus GV95 GPa |
Bulk Modulus KV165 GPa |
Shear Modulus GR66 GPa |
Bulk Modulus KR153 GPa |
Shear Modulus GVRH80 GPa |
Bulk Modulus KVRH159 GPa |
Elastic Anisotropy2.23 |
Poisson's Ratio0.28 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
6.06 | -0.00 | -0.00 |
-0.00 | 6.06 | -0.00 |
-0.00 | -0.00 | 4.58 |
Dielectric Tensor εij (total) |
||
---|---|---|
10.76 | -0.00 | -0.00 |
-0.00 | 10.76 | -0.00 |
-0.00 | -0.00 | 7.27 |
Polycrystalline dielectric constant
εpoly∞
5.56
|
Polycrystalline dielectric constant
εpoly
9.60
|
Refractive Index n2.36 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NiAuO2 (mp-997167) | 0.0602 | 0.001 | 3 |
AlCuO2 (mp-3098) | 0.0181 | 0.000 | 3 |
NiAuO2 (mp-997095) | 0.0504 | 0.000 | 3 |
CrPdO2 (mp-1063607) | 0.0634 | 0.000 | 3 |
CuAuO2 (mp-754126) | 0.0659 | 0.023 | 3 |
Explore more synthesis descriptions for materials of composition AlCuO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Al Cu_pv O |
Final Energy/Atom-6.5089 eV |
Corrected Energy-27.4403 eV
-27.4403 eV = -26.0357 eV (uncorrected energy) - 1.4046 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)