Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.966 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.007 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.96 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCa(CoO2)4 + CaO + La2O3 + O2 |
Band Gap0.123 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [148] |
Hall-R 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 0 1> | 234.6 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 322.6 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 205.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 117.3 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 351.9 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 138.5 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 205.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 156.3 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 234.4 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 166.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 29.3 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 117.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 29.3 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 322.6 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 29.3 |
BN (mp-984) | <0 0 1> | <0 0 1> | 88.0 |
BN (mp-984) | <1 1 0> | <0 0 1> | 264.0 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 117.3 |
Al (mp-134) | <1 0 0> | <0 0 1> | 146.6 |
Al (mp-134) | <1 1 0> | <0 0 1> | 117.3 |
Al (mp-134) | <1 1 1> | <0 0 1> | 29.3 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 322.6 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 234.6 |
TeO2 (mp-2125) | <1 0 1> | <1 0 0> | 78.1 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 322.6 |
TiO2 (mp-2657) | <1 0 0> | <1 0 1> | 83.5 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 78.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 264.0 |
C (mp-66) | <1 1 1> | <0 0 1> | 88.0 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 156.3 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 0> | 234.4 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 1> | 166.9 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 250.4 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 205.3 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 166.9 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 234.4 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 234.4 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 234.6 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 88.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 205.3 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 166.9 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 234.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 146.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 117.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 205.3 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 351.9 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 83.5 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 264.0 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 205.3 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 88.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Tl6TeO6 (mp-8387) | 0.5003 | 0.000 | 3 |
RbSnCl3 (mp-998611) | 0.4694 | 0.000 | 3 |
TlNiO3 (mp-998845) | 0.4571 | 0.284 | 3 |
Sr3TeO6 (mp-768907) | 0.2813 | 0.022 | 3 |
LaAgO3 (mp-768308) | 0.4298 | 0.035 | 3 |
CaLa2CrO6 (mvc-13419) | 0.1827 | 0.098 | 4 |
CaLa2FeO6 (mvc-13412) | 0.0607 | 0.090 | 4 |
CaLa2VO6 (mvc-11094) | 0.1573 | 0.041 | 4 |
CaLa2MnO6 (mvc-11030) | 0.1276 | 0.082 | 4 |
CaLa2TiO6 (mvc-13624) | 0.2524 | 0.063 | 4 |
Pb2O3 (mp-20078) | 0.7096 | 0.009 | 2 |
LuO3 (mp-1021512) | 0.6343 | 0.662 | 2 |
PtO2 (mp-1285) | 0.6721 | 0.000 | 2 |
CeSe2 (mp-1080328) | 0.6843 | 0.121 | 2 |
YbBr2 (mp-571232) | 0.7252 | 0.001 | 2 |
SrCoBiRuO6 (mp-743579) | 0.6469 | 0.171 | 5 |
SrLaMnMoO6 (mp-690552) | 0.6547 | 0.052 | 5 |
Sr5La3Mn4(WO6)4 (mp-694898) | 0.6671 | 0.038 | 5 |
SrLaMnRuO6 (mp-39239) | 0.6291 | 0.084 | 5 |
SrLaMnRuO6 (mp-690590) | 0.6750 | 0.084 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Ca_sv La Co O |
Final Energy/Atom-7.2237 eV |
Corrected Energy-155.9940 eV
Uncorrected energy = -144.4740 eV
Composition-based energy adjustment (-0.687 eV/atom x 12.0 atoms) = -8.2440 eV
Composition-based energy adjustment (-1.638 eV/atom x 2.0 atoms) = -3.2760 eV
Corrected energy = -155.9940 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)