Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.059 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.230 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.66 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCoS2 + Co3S4 + CaS |
Band Gap1.022 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI41/amd [141] |
HallI 4bw 2bw 1bw |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 293.9 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 249.6 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 220.4 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 249.6 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 293.9 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 199.7 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 266.5 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 266.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 349.4 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 177.7 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 199.7 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 249.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 199.7 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 249.6 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 293.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 207.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 249.6 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 349.4 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 349.4 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 88.8 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 220.4 |
Te2W (mp-22693) | <1 1 0> | <1 0 0> | 220.4 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 49.9 |
YVO4 (mp-19133) | <1 0 0> | <1 0 1> | 88.8 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 199.7 |
YVO4 (mp-19133) | <1 1 1> | <0 0 1> | 249.6 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 220.4 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 220.4 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 220.4 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 73.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 149.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 149.7 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 349.4 |
Al (mp-134) | <1 1 0> | <1 1 0> | 207.8 |
Al (mp-134) | <1 1 1> | <0 0 1> | 249.6 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 199.7 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 220.4 |
C (mp-66) | <1 1 0> | <1 0 0> | 73.5 |
C (mp-66) | <1 1 1> | <0 0 1> | 349.4 |
Mg (mp-153) | <1 0 0> | <1 0 1> | 266.5 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 249.6 |
BN (mp-984) | <0 0 1> | <0 0 1> | 349.4 |
BN (mp-984) | <1 0 0> | <0 0 1> | 149.7 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 73.5 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 0 1> | 149.7 |
KP(HO2)2 (mp-23959) | <1 0 0> | <1 0 0> | 220.4 |
LaF3 (mp-905) | <0 0 1> | <1 0 1> | 88.8 |
LaF3 (mp-905) | <1 0 1> | <1 0 1> | 266.5 |
MoS2 (mp-1434) | <1 0 0> | <1 0 1> | 266.5 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 249.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca(CoS2)2 (mvc-12728) | 0.1503 | 0.229 | 3 |
Y(CoS2)2 (mvc-16744) | 0.1228 | 0.332 | 3 |
Ca(FeS2)2 (mvc-14056) | 0.1375 | 0.367 | 3 |
Ca(FeS2)2 (mvc-11254) | 0.0978 | 0.282 | 3 |
Al2HgO4 (mp-756317) | 0.1348 | 0.087 | 3 |
Li2Mn3NbO8 (mp-775745) | 0.5720 | 0.060 | 4 |
LiCuTeO4 (mp-755347) | 0.5629 | 0.069 | 4 |
LiMnVO4 (mp-774424) | 0.5444 | 0.061 | 4 |
LiMnNbO4 (mp-772258) | 0.5784 | 0.000 | 4 |
LiVCoO4 (mp-761722) | 0.5824 | 0.031 | 4 |
Pu2O3 (mp-637224) | 0.6296 | 0.000 | 2 |
NiS2 (mp-850068) | 0.5359 | 0.097 | 2 |
Co3O4 (mp-559191) | 0.6288 | 0.010 | 2 |
Mn3O4 (mp-18759) | 0.6275 | 0.000 | 2 |
Mg3P2 (mp-2514) | 0.6225 | 0.000 | 2 |
Li4V2Cr3Fe3O16 (mp-770523) | 0.7413 | 0.892 | 5 |
Li4V2Co3Cu3O16 (mp-763156) | 0.7486 | 0.079 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv Co S |
Final Energy/Atom-5.3611 eV |
Corrected Energy-80.3631 eV
-80.3631 eV = -75.0555 eV (uncorrected energy) - 5.3077 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)