Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.093 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.39 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.087 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [148] |
Hall-R 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 1> | <0 0 1> | 124.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 24.9 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 249.4 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 174.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 174.6 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 223.4 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 249.4 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 124.7 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 74.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 157.1 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 297.9 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 324.3 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 174.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 374.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 324.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 174.6 |
TePb (mp-19717) | <1 0 0> | <1 1 1> | 131.4 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 74.8 |
Ag (mp-124) | <1 0 0> | <1 1 0> | 258.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 224.5 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 24.9 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 74.8 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 223.4 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 199.6 |
BN (mp-984) | <1 0 0> | <0 0 1> | 324.3 |
BN (mp-984) | <1 0 1> | <0 0 1> | 224.5 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 148.9 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 297.9 |
LiNbO3 (mp-3731) | <1 0 1> | <1 0 1> | 78.5 |
LiNbO3 (mp-3731) | <1 1 0> | <1 1 0> | 129.0 |
MoS2 (mp-1434) | <1 0 0> | <0 0 1> | 199.6 |
MoS2 (mp-1434) | <1 1 0> | <1 0 0> | 223.4 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 148.9 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 148.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 299.3 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 299.3 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 249.4 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 223.4 |
CdTe (mp-406) | <1 0 0> | <1 1 1> | 131.4 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 299.3 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 157.1 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 24.9 |
SiC (mp-7631) | <1 1 0> | <0 0 1> | 249.4 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 199.6 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 299.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 74.8 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 314.1 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 324.3 |
BN (mp-984) | <0 0 1> | <1 0 0> | 223.4 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 24.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.52 | -0.00 | -0.00 |
-0.00 | 2.52 | -0.00 |
-0.00 | -0.00 | 2.46 |
Dielectric Tensor εij (total) |
||
---|---|---|
3.27 | -0.00 | -0.00 |
-0.00 | 3.27 | -0.00 |
-0.00 | -0.00 | 3.08 |
Polycrystalline dielectric constant
εpoly∞
2.50
|
Polycrystalline dielectric constant
εpoly
3.21
|
Refractive Index n1.58 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
OsOF5 (mp-504576) | 0.4626 | 0.000 | 3 |
Ru(OF3)2 (mp-505242) | 0.5645 | 0.000 | 3 |
AsIF12 (mp-555340) | 0.2834 | 0.000 | 3 |
OsOF5 (mp-555514) | 0.4653 | 0.000 | 3 |
SbSNF6 (mp-683956) | 0.6755 | 0.101 | 4 |
Na2H6PtO6 (mp-632760) | 0.7260 | 0.000 | 4 |
Na2Hf(HO)6 (mp-643896) | 0.7009 | 0.018 | 4 |
AsS(IF3)2 (mp-557628) | 0.6173 | 0.000 | 4 |
TeAs(ClF2)3 (mp-556325) | 0.7378 | 0.000 | 4 |
SF6 (mp-975) | 0.2749 | 0.001 | 2 |
TeF6 (mvc-15700) | 0.0485 | 0.001 | 2 |
SF6 (mp-642824) | 0.2151 | 0.007 | 2 |
SF6 (mp-8652) | 0.2618 | 0.002 | 2 |
WCl6 (mp-571518) | 0.2568 | 0.000 | 2 |
Run TypeGGA+U |
Energy Cutoff700 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Cr_pv F |
Final Energy/Atom-4.4016 eV |
Corrected Energy-32.8242 eV
-32.8242 eV = -30.8112 eV (uncorrected energy) - 2.0130 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)