Final Magnetic Moment7.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.518 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.126 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.28 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCr2O3 + Al2O3 + Cr |
Band Gap2.084 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [166] |
Hall-R 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 213.0 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 273.8 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 243.4 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 213.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 334.7 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 334.7 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 213.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 365.1 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 121.7 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 121.7 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 213.0 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 213.0 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 334.7 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 243.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 273.8 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 173.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 334.7 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 30.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 91.3 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 273.8 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 91.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 365.1 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 273.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 243.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 152.1 |
Al (mp-134) | <1 0 0> | <0 0 1> | 243.4 |
Al (mp-134) | <1 1 1> | <0 0 1> | 365.1 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 334.7 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 30.4 |
YVO4 (mp-19133) | <0 0 1> | <1 1 1> | 153.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 213.0 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 273.8 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 121.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 121.7 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 91.3 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 91.3 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 30.4 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 273.8 |
BN (mp-984) | <0 0 1> | <0 0 1> | 213.0 |
BN (mp-984) | <1 0 1> | <0 0 1> | 213.0 |
BN (mp-984) | <1 1 0> | <0 0 1> | 273.8 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 173.5 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 334.7 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 273.8 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 182.5 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 365.1 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 0> | 260.3 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 0> | 173.5 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 273.8 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 91.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ti2AlO4 (mvc-10896) | 0.1434 | 0.064 | 3 |
AlV2O4 (mvc-11436) | 0.1082 | 0.058 | 3 |
Al(FeO2)2 (mvc-10947) | 0.1463 | 0.539 | 3 |
Ti2AlO4 (mvc-11532) | 0.1478 | 0.064 | 3 |
Mn2AlO4 (mvc-11435) | 0.1401 | 0.121 | 3 |
LiVNiO4 (mp-771631) | 0.1615 | 0.001 | 4 |
Li7V6Ni5O24 (mp-769574) | 0.2051 | 0.013 | 4 |
LiMnVO4 (mp-861571) | 0.2307 | 0.024 | 4 |
LiVFeO4 (mp-773535) | 0.2294 | 0.016 | 4 |
LiVCoO4 (mp-768046) | 0.1675 | 0.000 | 4 |
Fe3S4 (mp-21515) | 0.2422 | 0.197 | 2 |
Fe3O4 (mp-715490) | 0.2305 | 0.000 | 2 |
Cr3N4 (mp-1014379) | 0.2153 | 0.105 | 2 |
Fe3O4 (mp-715558) | 0.2569 | 0.785 | 2 |
Fe3O4 (mp-715811) | 0.2586 | 0.037 | 2 |
Li2Cr2FeSbO8 (mp-861530) | 0.3904 | 0.802 | 5 |
Li4Ti3Cr3(WO8)2 (mp-773537) | 0.3912 | 0.046 | 5 |
Li4Cr3Fe3(TeO8)2 (mp-773518) | 0.3851 | 1.173 | 5 |
Li4Fe3Ni3(TeO8)2 (mp-773382) | 0.3808 | 0.197 | 5 |
Li4Cr3Fe3(SbO8)2 (mp-771925) | 0.3724 | 0.871 | 5 |
Li3MnFeCo(PO4)3 (mp-764931) | 0.6026 | 0.017 | 6 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.5943 | 0.014 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.5982 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764707) | 0.6042 | 0.035 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.5934 | 0.057 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Al Cr_pv O |
Final Energy/Atom-7.6623 eV |
Corrected Energy-120.9432 eV
-120.9432 eV = -107.2728 eV (uncorrected energy) - 8.0520 eV (MP Advanced Correction) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)