Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.980 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.037 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.56 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTiFeO3 + CaTiO3 |
Band Gap1.790 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinIm3 [204] |
Hall-I 2 2 3 |
Point Groupm3 |
Crystal Systemcubic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <1 1 1> | 296.1 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 170.9 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 284.9 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 161.2 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 170.9 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 241.7 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 296.1 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 170.9 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 284.9 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 341.9 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 284.9 |
Te2W (mp-22693) | <0 0 1> | <1 1 1> | 197.4 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 161.2 |
Te2Mo (mp-602) | <0 0 1> | <1 1 1> | 98.7 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 161.2 |
BN (mp-984) | <1 0 0> | <1 0 0> | 57.0 |
BN (mp-984) | <1 1 0> | <1 0 0> | 227.9 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 1> | 296.1 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 284.9 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 170.9 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 0> | 241.7 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 227.9 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 241.7 |
CdTe (mp-406) | <1 1 1> | <1 1 1> | 296.1 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 284.9 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 227.9 |
SiC (mp-7631) | <1 0 1> | <1 0 0> | 227.9 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 0> | 284.9 |
LiTaO3 (mp-3666) | <1 0 0> | <1 1 1> | 296.1 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 284.9 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 284.9 |
MgO (mp-1265) | <1 1 1> | <1 0 0> | 284.9 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 284.9 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 341.9 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 114.0 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <1 1 0> | 161.2 |
C (mp-66) | <1 0 0> | <1 0 0> | 114.0 |
C (mp-66) | <1 1 0> | <1 1 0> | 161.2 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 284.9 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 170.9 |
Mg (mp-153) | <1 1 0> | <1 1 1> | 296.1 |
Mg (mp-153) | <1 1 1> | <1 1 0> | 241.7 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 284.9 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 241.7 |
CeO2 (mp-20194) | <1 0 0> | <1 1 1> | 296.1 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 284.9 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 227.9 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 227.9 |
KP(HO2)2 (mp-23959) | <1 0 0> | <1 0 0> | 114.0 |
LaF3 (mp-905) | <1 0 0> | <1 1 0> | 161.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiMn7O12 (mp-769733) | 0.3033 | 0.061 | 3 |
Li3CuF6 (mp-760812) | 0.2623 | 0.045 | 3 |
NaMn7O12 (mp-18999) | 0.3490 | 0.029 | 3 |
YCu7O12 (mvc-1832) | 0.3294 | 0.000 | 3 |
AlCu7O12 (mvc-1846) | 0.3194 | 0.209 | 3 |
CaV4(CuO4)3 (mp-542267) | 0.2340 | 0.075 | 4 |
CaTi4(FeO4)3 (mvc-11639) | 0.0044 | 0.037 | 4 |
ZnCu3(WO3)4 (mvc-8372) | 0.2394 | 0.252 | 4 |
CaCu3(GeO3)4 (mvc-16384) | 0.1555 | 0.094 | 4 |
CaCu3(GeO3)4 (mp-17599) | 0.2179 | 0.094 | 4 |
CaNb2Ga2(CuO4)3 (mp-686705) | 0.3741 | 0.111 | 5 |
CaTa2Ga2(CuO4)3 (mp-694913) | 0.3587 | 0.000 | 5 |
CaGa2Cu3(SbO6)2 (mp-41331) | 0.3572 | 0.080 | 5 |
NdTi3Fe(CuO4)3 (mp-690601) | 0.3691 | 0.046 | 5 |
NdTi3Fe(CuO4)3 (mp-39888) | 0.3699 | 0.046 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Ca_sv Ti_pv Fe_pv O |
Final Energy/Atom-8.0671 eV |
Corrected Energy-352.7079 eV
Uncorrected energy = -322.6839 eV
Composition-based energy adjustment (-0.687 eV/atom x 24.0 atoms) = -16.4880 eV
Composition-based energy adjustment (-2.256 eV/atom x 6.0 atoms) = -13.5360 eV
Corrected energy = -352.7079 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)