Final Magnetic Moment0.101 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.965 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.188 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.00 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBiO2 + Mg3(AsO4)2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm [6] |
HallP 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 202.6 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 -1> | 307.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 202.6 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 201.6 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 252.0 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 81.1 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 201.6 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 41.3 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 206.5 |
GaAs (mp-2534) | <1 0 0> | <1 0 -1> | 131.6 |
GaAs (mp-2534) | <1 1 1> | <1 0 -1> | 219.3 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 -1> | 219.3 |
CeO2 (mp-20194) | <1 0 0> | <1 0 -1> | 87.7 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 258.7 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 130.3 |
GaN (mp-804) | <1 1 0> | <1 0 -1> | 87.7 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 121.6 |
GaAs (mp-2534) | <1 1 0> | <0 1 1> | 323.4 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 165.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 243.2 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 81.1 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 325.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 123.9 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 162.1 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 123.9 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 243.2 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 260.7 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 175.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 -1> | 131.6 |
ZnSe (mp-1190) | <1 1 0> | <0 1 1> | 323.4 |
ZnSe (mp-1190) | <1 1 1> | <1 0 -1> | 219.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 -1> | 43.9 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 162.1 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 323.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 -1> | 131.6 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 151.2 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 324.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 131.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 323.4 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 -1> | 350.9 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 121.6 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 201.6 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 202.6 |
CdS (mp-672) | <1 1 1> | <1 0 -1> | 263.2 |
LiF (mp-1138) | <1 0 0> | <1 0 -1> | 131.6 |
LiF (mp-1138) | <1 1 0> | <1 0 -1> | 307.1 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 162.1 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 283.7 |
YVO4 (mp-19133) | <1 1 1> | <0 1 1> | 258.7 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 283.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SnPO4 (mp-673078) | 0.5951 | 0.175 | 3 |
Li2Cr2O7 (mp-772297) | 0.6367 | 0.072 | 3 |
Na2Si2O5 (mp-556307) | 0.7175 | 0.001 | 3 |
CaMo2O7 (mvc-7390) | 0.7193 | 0.111 | 3 |
MgCr2O7 (mvc-7371) | 0.6994 | 1.234 | 3 |
Mg3V2(BiO6)2 (mvc-13124) | 0.1376 | 0.175 | 4 |
Mg3Bi2(PO6)2 (mvc-11923) | 0.2921 | 0.167 | 4 |
Mg3Bi2(PO6)2 (mvc-12806) | 0.3359 | 0.180 | 4 |
Zn3Bi2(PO6)2 (mvc-11996) | 0.4640 | 0.131 | 4 |
MgSnP2O7 (mvc-980) | 0.6203 | 0.039 | 4 |
Li4V5CuClO15 (mp-769746) | 0.7461 | 0.059 | 5 |
ZnGaP2H4NO8 (mp-693132) | 0.7287 | 0.032 | 6 |
NaCaMgAl(SiO3)4 (mp-720244) | 0.7329 | 0.317 | 6 |
Al3P3H9C2NO13 (mp-772922) | 0.7096 | 0.036 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv Bi As O |
Final Energy/Atom-5.7976 eV |
Corrected Energy-118.5823 eV
-118.5823 eV = -110.1549 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)