Final Magnetic Moment6.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.474 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.122 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.05 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCa3Ga4O9 + Ca2Mn3O8 + CaO |
Band Gap0.224 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPc [7] |
HallP 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 154.2 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 215.8 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 244.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 154.2 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 123.3 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 92.5 |
GaAs (mp-2534) | <1 1 1> | <1 0 -1> | 228.9 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 163.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 215.8 |
GaN (mp-804) | <1 1 0> | <1 0 -1> | 228.9 |
GaN (mp-804) | <1 1 1> | <1 0 -1> | 152.6 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 154.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 81.5 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 30.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 163.0 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 339.2 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 81.5 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 228.9 |
CeO2 (mp-20194) | <1 0 0> | <1 0 -1> | 152.6 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 81.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 1> | 125.7 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 92.5 |
ZnSe (mp-1190) | <1 1 1> | <1 0 -1> | 228.9 |
GaN (mp-804) | <1 0 0> | <1 1 1> | 251.3 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 277.5 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 277.5 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 92.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 277.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 92.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 277.5 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 215.8 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 92.5 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 215.8 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 163.0 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 244.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 277.5 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 308.3 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 277.5 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 228.6 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 246.7 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 92.5 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 277.5 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 339.2 |
Te2W (mp-22693) | <0 1 1> | <1 0 -1> | 228.9 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 277.5 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 163.0 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 163.0 |
BN (mp-984) | <0 0 1> | <0 0 1> | 246.7 |
BN (mp-984) | <1 0 1> | <0 0 1> | 277.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 246.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na8Gd2O7 (mp-780360) | 0.6964 | 0.080 | 3 |
CaGe2O5 (mp-554678) | 0.6438 | 0.014 | 3 |
Li8Fe2O7 (mp-781076) | 0.7415 | 0.089 | 3 |
Ba8In8O19 (mp-757574) | 0.4503 | 0.017 | 3 |
CdGe2O5 (mp-7762) | 0.6543 | 0.013 | 3 |
CaMnFeO5 (mvc-12807) | 0.5131 | 0.233 | 4 |
Ca3Mn2(FeO5)2 (mvc-13130) | 0.1713 | 0.135 | 4 |
Ca6Mn3Al2O15 (mvc-12222) | 0.5429 | 0.099 | 4 |
Ca3Mn2(GaO5)2 (mvc-12044) | 0.1893 | 0.120 | 4 |
Ca3Ga2(FeO5)2 (mvc-15035) | 0.2538 | 0.083 | 4 |
Li6MnV3(PO4)6 (mp-764743) | 0.6097 | 0.044 | 5 |
Li3MnV(PO4)3 (mp-779371) | 0.6629 | 0.056 | 5 |
Li3MnV(PO4)3 (mp-779177) | 0.6364 | 0.055 | 5 |
Ca7MgFeCo7O20 (mp-1099907) | 0.6261 | 0.075 | 5 |
Ca7MgCo7CuO20 (mp-1099952) | 0.6168 | 0.088 | 5 |
Ca10Ti8NbAl(SiO5)10 (mp-693409) | 0.6722 | 0.004 | 6 |
Ca6Ti5AlSi6O29F (mp-693358) | 0.6471 | 0.007 | 6 |
Ca10Ta3Ti4Al3(SiO5)10 (mp-534838) | 0.6721 | 0.006 | 6 |
NaCa9Ti9Nb(SiO5)10 (mp-534850) | 0.6692 | 0.000 | 6 |
Ca5TaTi3Al(SiO5)5 (mp-720394) | 0.6757 | 0.000 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Ca_sv Mn_pv Ga_d O |
Final Energy/Atom-6.5621 eV |
Corrected Energy-243.8811 eV
-243.8811 eV = -223.1119 eV (uncorrected energy) - 14.0458 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)