Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.913 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.049 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.84 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCa(CoO2)2 |
Band Gap2.323 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFd3m [227] |
HallF 4d 2 3 1d |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 287.5 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 215.6 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 143.8 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 101.7 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 287.5 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 143.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 203.3 |
LiF (mp-1138) | <1 0 0> | <1 1 1> | 249.0 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 215.6 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 287.5 |
TeO2 (mp-2125) | <0 1 0> | <1 1 0> | 203.3 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 203.3 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 287.5 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 71.9 |
Fe3O4 (mp-19306) | <1 1 0> | <1 1 0> | 101.7 |
Fe3O4 (mp-19306) | <1 1 1> | <1 1 1> | 124.5 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 71.9 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 101.7 |
MgO (mp-1265) | <1 1 1> | <1 1 1> | 124.5 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 287.5 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 287.5 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 287.5 |
ZnO (mp-2133) | <1 0 1> | <1 0 0> | 215.6 |
ZnO (mp-2133) | <1 1 1> | <1 0 0> | 287.5 |
Ge (mp-32) | <1 0 0> | <1 0 0> | 287.5 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 71.9 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 101.7 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 71.9 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 101.7 |
Ni (mp-23) | <1 1 1> | <1 0 0> | 215.6 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 143.8 |
BaTiO3 (mp-5986) | <1 0 0> | <1 1 0> | 101.7 |
MoSe2 (mp-1634) | <0 0 1> | <1 1 1> | 124.5 |
C (mp-48) | <1 0 0> | <1 0 0> | 287.5 |
WSe2 (mp-1821) | <0 0 1> | <1 1 1> | 124.5 |
NaCl (mp-22862) | <1 0 0> | <1 0 0> | 287.5 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 287.5 |
CdWO4 (mp-19387) | <1 0 0> | <1 1 1> | 124.5 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 71.9 |
MgF2 (mp-1249) | <0 0 1> | <1 0 0> | 287.5 |
SrTiO3 (mp-4651) | <0 0 1> | <1 0 0> | 287.5 |
Cu (mp-30) | <1 1 0> | <1 1 0> | 203.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Y(CoS2)2 (mvc-16744) | 0.1030 | 0.332 | 3 |
Ca(NiO2)2 (mvc-14927) | 0.0830 | 0.082 | 3 |
Co2HgO4 (mp-769697) | 0.0799 | 0.044 | 3 |
NaCr2O4 (mp-849216) | 0.0959 | 0.091 | 3 |
Cr2HgO4 (mp-24899) | 0.0900 | 0.000 | 3 |
Li2Mn3NbO8 (mp-775745) | 0.5038 | 0.060 | 4 |
LiMnVO4 (mp-774424) | 0.5189 | 0.061 | 4 |
LiCoNiO4 (mp-776511) | 0.5173 | 0.000 | 4 |
Li2Co3NiO8 (mp-761738) | 0.5134 | 0.226 | 4 |
Li2MnFe3O8 (mp-775094) | 0.5181 | 0.095 | 4 |
Mn3O4 (mp-566607) | 0.6046 | 0.000 | 2 |
NiS2 (mp-850068) | 0.5972 | 0.097 | 2 |
Co3O4 (mp-559191) | 0.4916 | 0.010 | 2 |
Mn3O4 (mp-18759) | 0.6029 | 0.000 | 2 |
Co3O4 (mp-18748) | 0.5167 | 0.010 | 2 |
Li4Nb2V3Fe3O16 (mp-762676) | 0.7211 | 0.020 | 5 |
Li4V2Cr3Fe3O16 (mp-770523) | 0.7022 | 0.892 | 5 |
Li4V3Ni3(WO8)2 (mp-777059) | 0.7057 | 0.032 | 5 |
Li4V2Co3Cu3O16 (mp-763156) | 0.7105 | 0.079 | 5 |
Li4V3Co3(WO8)2 (mp-763152) | 0.7191 | 0.263 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Ca_sv Co O |
Final Energy/Atom-6.1210 eV |
Corrected Energy-98.8086 eV
-98.8086 eV = -85.6943 eV (uncorrected energy) - 7.4960 eV (MP Advanced Correction) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)