material

MnO2

ID:

mp-19395

DOI:

10.17188/1194402


Material Details

Final Magnetic Moment
3.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-1.806 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.01 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
1.169 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4/m [87]
Hall
-I 4
Point Group
4/m
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 20227 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ni (mp-23) <1 0 0> <0 0 1> 0.000 98.5
BaF2 (mp-1029) <1 0 0> <0 0 1> 0.002 197.0
AlN (mp-661) <0 0 1> <1 1 0> 0.008 287.8
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.019 197.0
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.055 197.0
SiO2 (mp-6930) <1 0 1> <1 1 1> 0.059 106.7
BN (mp-984) <1 1 0> <1 0 0> 0.062 232.5
Ga2O3 (mp-886) <1 0 0> <1 1 0> 0.070 164.4
BaTiO3 (mp-5986) <1 0 1> <1 0 0> 0.070 116.3
LaAlO3 (mp-2920) <0 0 1> <1 1 0> 0.082 328.9
TiO2 (mp-390) <0 0 1> <1 1 0> 0.086 287.8
C (mp-66) <1 0 0> <1 0 1> 0.094 102.7
PbSe (mp-2201) <1 0 0> <0 0 1> 0.108 197.0
Fe2O3 (mp-24972) <1 0 0> <1 1 1> 0.115 213.5
MoSe2 (mp-1634) <0 0 1> <1 1 0> 0.116 123.3
WSe2 (mp-1821) <0 0 1> <1 1 0> 0.116 123.3
BN (mp-984) <0 0 1> <1 0 0> 0.123 87.2
InAs (mp-20305) <1 1 1> <1 0 0> 0.129 261.6
SiO2 (mp-6930) <0 0 1> <1 0 0> 0.133 87.2
ZnTe (mp-2176) <1 1 1> <1 0 0> 0.135 261.6
CdWO4 (mp-19387) <1 1 1> <1 1 0> 0.135 205.5
CaCO3 (mp-3953) <0 0 1> <1 0 0> 0.141 87.2
GaSb (mp-1156) <1 0 0> <0 0 1> 0.144 197.0
Ag (mp-124) <1 1 1> <0 0 1> 0.146 295.5
C (mp-66) <1 1 1> <1 0 0> 0.150 87.2
CdS (mp-672) <1 0 1> <1 0 0> 0.158 232.5
Cu (mp-30) <1 1 0> <1 0 0> 0.162 261.6
CdWO4 (mp-19387) <0 1 0> <1 0 0> 0.165 319.7
GdScO3 (mp-5690) <1 0 0> <1 0 0> 0.166 232.5
Bi2Te3 (mp-34202) <0 0 1> <1 1 0> 0.170 328.9
C (mp-48) <0 0 1> <1 1 0> 0.173 246.6
CdSe (mp-2691) <1 0 0> <0 0 1> 0.176 197.0
ZnO (mp-2133) <0 0 1> <1 1 0> 0.177 123.3
MgF2 (mp-1249) <1 0 0> <1 1 0> 0.184 328.9
BaTiO3 (mp-5986) <1 0 0> <1 0 0> 0.188 203.5
ZnO (mp-2133) <1 0 0> <1 0 0> 0.195 319.7
ZnO (mp-2133) <1 0 1> <1 0 0> 0.199 319.7
SiC (mp-11714) <0 0 1> <1 0 0> 0.202 319.7
MgF2 (mp-1249) <1 0 1> <1 0 0> 0.203 348.8
TiO2 (mp-2657) <1 1 0> <1 0 0> 0.204 58.1
SiC (mp-7631) <0 0 1> <1 0 0> 0.207 319.7
TiO2 (mp-2657) <1 0 0> <1 1 0> 0.207 41.1
CdS (mp-672) <1 1 1> <1 1 0> 0.217 205.5
Fe2O3 (mp-24972) <1 1 0> <1 1 0> 0.218 123.3
Au (mp-81) <1 1 1> <0 0 1> 0.228 295.5
CdSe (mp-2691) <1 1 1> <1 0 0> 0.232 261.6
AlN (mp-661) <1 0 0> <1 0 0> 0.247 261.6
TbScO3 (mp-31119) <1 0 0> <1 0 0> 0.262 232.5
GaSb (mp-1156) <1 1 1> <1 0 0> 0.266 261.6
C (mp-48) <1 0 1> <1 0 0> 0.282 203.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.

Once you have registered you can also "vote" for full calculation of this material's elastic properties.

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
10.04 0.00 -0.00
0.00 7.97 0.00
-0.00 -0.00 7.97
Dielectric Tensor εij (total)
16.41 0.00 -0.00
0.00 13.03 0.00
-0.00 -0.00 13.03
Polycrystalline dielectric constant εpoly
(electronic contribution)
8.66
Polycrystalline dielectric constant εpoly
(total)
14.16
Refractive Index n
2.94
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ni3OF5 (mp-763929) 0.2549 0.072 3
Ni6OF11 (mp-853157) 0.2635 0.036 3
Mn3O5F (mp-777654) 0.2612 0.062 3
Ni3OF5 (mp-763299) 0.2596 0.066 3
Ni3OF5 (mp-765774) 0.2572 0.075 3
LiFe3(OF3)2 (mp-779990) 0.3100 0.007 4
LiV3(OF3)2 (mp-868491) 0.2758 0.000 4
LiFe2OF5 (mp-779300) 0.3379 0.054 4
LiCo3(OF3)2 (mp-850982) 0.2795 0.024 4
Ta2CrNO5 (mp-849504) 0.2978 0.063 4
FeO2 (mvc-12905) 0.1470 0.180 2
CrO2 (mvc-12040) 0.1591 0.066 2
MnO2 (mvc-12022) 0.0205 0.000 2
SnO2 (mvc-15363) 0.1202 0.069 2
CoO2 (mvc-14149) 0.1173 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

All chemicals were obtained commercially and used as received without further purification. The pure MnO2 was synthesized by a typical hydrothermal synthesis. 0.6mmol of MnCl24H2O and 1.8mmol of KM [...]
All the chemical reagents were of analytical purity and used without any further purification. Nest-like MnO2 hollow nanospheres were prepared via a facile hydrothermal process as follows. An amount o [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition MnO2.

Text computed by synthesisproject.org.

Calculation Summary

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
Mn: 3.9 eV
Pseudopotentials
VASP PAW: Mn_pv O
Final Energy/Atom
-7.1445 eV
Corrected Energy
-97.9017 eV
Uncorrected energy = -85.7337 eV Composition-based energy adjustment (-0.687 eV/atom x 8.0 atoms) = -5.4960 eV Composition-based energy adjustment (-1.668 eV/atom x 4.0 atoms) = -6.6720 eV Corrected energy = -97.9017 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation