Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.051 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.074 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.07 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCu2O3 + V2O5 + CaV2O6 |
Band Gap0.638 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP2 [3] |
HallP 2y |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 283.2 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 283.2 |
BaF2 (mp-1029) | <1 1 1> | <1 0 1> | 132.8 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 217.6 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 132.8 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 283.2 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 272.1 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 272.1 |
InAs (mp-20305) | <1 1 1> | <1 0 1> | 132.8 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 283.2 |
Te2Mo (mp-602) | <1 0 0> | <1 0 1> | 265.6 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 272.1 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 272.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 272.1 |
BN (mp-984) | <0 0 1> | <1 0 0> | 283.2 |
BN (mp-984) | <1 1 0> | <1 0 1> | 132.8 |
BN (mp-984) | <1 1 1> | <0 0 1> | 272.1 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 272.1 |
SiC (mp-11714) | <1 1 0> | <0 0 1> | 272.1 |
Ga2O3 (mp-886) | <1 1 1> | <1 1 1> | 171.7 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 272.1 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 272.1 |
ZrO2 (mp-2858) | <1 0 0> | <1 0 0> | 283.2 |
CaCO3 (mp-3953) | <0 0 1> | <1 0 1> | 132.8 |
CaCO3 (mp-3953) | <1 0 0> | <1 0 1> | 265.6 |
YAlO3 (mp-3792) | <1 1 1> | <0 0 1> | 181.4 |
SiC (mp-8062) | <1 1 0> | <0 0 1> | 272.1 |
TiO2 (mp-390) | <1 0 1> | <0 0 1> | 272.1 |
MgF2 (mp-1249) | <1 1 0> | <1 0 1> | 265.6 |
ZnO (mp-2133) | <1 0 0> | <1 0 0> | 283.2 |
GaSb (mp-1156) | <1 1 0> | <0 0 1> | 272.1 |
GaSb (mp-1156) | <1 1 1> | <1 0 1> | 132.8 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 90.7 |
LiAlO2 (mp-3427) | <0 0 1> | <0 0 1> | 272.1 |
Fe2O3 (mp-24972) | <0 0 1> | <0 0 1> | 90.7 |
ZnTe (mp-2176) | <1 1 0> | <0 0 1> | 272.1 |
ZnTe (mp-2176) | <1 1 1> | <1 0 1> | 132.8 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 94.4 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 272.1 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 283.2 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 272.1 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 272.1 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 0> | 94.4 |
C (mp-66) | <1 1 1> | <1 0 1> | 132.8 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 283.2 |
LaF3 (mp-905) | <1 0 0> | <0 1 0> | 108.8 |
LaF3 (mp-905) | <1 0 1> | <0 0 1> | 272.1 |
PbSe (mp-2201) | <1 1 1> | <1 0 1> | 132.8 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 0> | 217.6 |
MoSe2 (mp-1634) | <1 1 1> | <1 0 1> | 265.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaCr2CuO7 (mvc-6899) | 0.7326 | 0.118 | 4 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Ca_sv V_pv Cu_pv O |
Final Energy/Atom-6.7768 eV |
Corrected Energy-476.6159 eV
-476.6159 eV = -426.9357 eV (uncorrected energy) - 29.4962 eV (MP Anion Correction) - 20.1840 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)