Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-1.627 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.167 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.18 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCr5O12 + O2 |
Band Gap0.544 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPmmn [59] |
HallP 2 2ab 1ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 278.8 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 331.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 209.1 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 131.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 278.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 209.1 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 200.7 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 243.9 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 199.2 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 321.1 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 209.1 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 120.4 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 331.9 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 200.7 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 278.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 348.5 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 264.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 331.9 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 278.4 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 278.8 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 261.4 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 211.5 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 132.8 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 205.9 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 120.4 |
InAs (mp-20305) | <1 0 0> | <0 1 1> | 218.8 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 265.5 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 240.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 243.9 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 281.0 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 265.5 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 200.7 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 278.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 200.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 243.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 313.6 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 104.5 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 313.6 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 331.1 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 243.9 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 160.6 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 200.7 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 265.5 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 313.6 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 226.5 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 174.2 |
Te2W (mp-22693) | <1 0 0> | <1 0 1> | 278.4 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 160.6 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 139.4 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 69.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.65 | 0.00 | 0.00 |
0.00 | 6.87 | 0.00 |
0.00 | 0.00 | 7.61 |
Dielectric Tensor εij (total) |
||
---|---|---|
4.31 | 0.00 | 0.00 |
0.00 | 13.33 | 0.00 |
0.00 | 0.00 | 18.22 |
Polycrystalline dielectric constant
εpoly∞
6.04
|
Polycrystalline dielectric constant
εpoly
11.95
|
Refractive Index n2.46 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnW2O5 (mvc-4941) | 0.4513 | 0.592 | 3 |
V2MoO8 (mp-561475) | 0.6108 | 0.030 | 3 |
VHgO3 (mp-541588) | 0.7141 | 0.000 | 3 |
ZnMo2O5 (mvc-5304) | 0.5830 | 0.566 | 3 |
VAgSeO5 (mp-605905) | 0.7072 | 0.000 | 4 |
V2O5 (mp-849597) | 0.2900 | 0.009 | 2 |
V2O5 (mvc-11647) | 0.3436 | 0.011 | 2 |
V2O5 (mp-543104) | 0.2515 | 0.009 | 2 |
Cr2O5 (mvc-12540) | 0.0601 | 0.167 | 2 |
V2O5 (mvc-11944) | 0.2904 | 0.000 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Cr_pv O |
Final Energy/Atom-6.8430 eV |
Corrected Energy-110.8763 eV
-110.8763 eV = -95.8014 eV (uncorrected energy) - 8.0520 eV (MP Advanced Correction) - 7.0229 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)