Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.461 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.387 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.46 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSbO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [166] |
Hall-R 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 313.4 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 131.4 |
AlN (mp-661) | <1 0 0> | <1 1 1> | 248.2 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 192.1 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 272.9 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 171.8 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 237.1 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 339.4 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 161.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 101.1 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 141.5 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 189.7 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 283.0 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 70.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 121.3 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 237.1 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 212.3 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 232.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 91.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 192.1 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 142.2 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 283.0 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 70.8 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 272.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 202.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 192.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 131.4 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 202.2 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 293.1 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 242.6 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 313.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 161.7 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 333.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 50.5 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 121.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 30.3 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 141.5 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 283.0 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 189.7 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 192.1 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 101.1 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 141.5 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 161.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 182.0 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 193.9 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 161.7 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 237.1 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 192.1 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 323.5 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 212.3 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
203 | 103 | 35 | 6 | 0 | 0 |
103 | 203 | 35 | -6 | 0 | 0 |
35 | 35 | 2 | 0 | 0 | 0 |
6 | -6 | 0 | 17 | 0 | 0 |
0 | 0 | 0 | 0 | 17 | 6 |
0 | 0 | 0 | 0 | 6 | 50 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
4.6 | -5.9 | 19.6 | -4.1 | 0.0 | 0.0 |
-5.9 | 4.6 | 19.6 | 4.1 | -0.0 | 0.0 |
19.6 | 19.6 | -170.9 | -0.0 | 0.0 | -0.0 |
-4.1 | 4.1 | -0.0 | 63.0 | -0.0 | 0.0 |
0.0 | -0.0 | 0.0 | -0.0 | 63.0 | -8.1 |
0.0 | 0.0 | -0.0 | 0.0 | -8.1 | 21.0 |
Shear Modulus GV32 GPa |
Bulk Modulus KV84 GPa |
Shear Modulus GR-44 GPa |
Bulk Modulus KR-11 GPa |
Shear Modulus GVRH-6 GPa |
Bulk Modulus KVRH37 GPa |
Elastic Anisotropy-17.63 |
Poisson's Ratio0.59 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TiNbO4 (mp-755302) | 0.5655 | 0.054 | 3 |
TiVO4 (mp-780818) | 0.5550 | 0.043 | 3 |
CrSbO4 (mp-771809) | 0.4801 | 0.120 | 3 |
Ca3SiBr2 (mp-570032) | 0.5165 | 0.192 | 3 |
Mn3SbO8 (mp-776354) | 0.5364 | 0.100 | 3 |
LiFe5(OF2)4 (mp-782691) | 0.7347 | 0.081 | 4 |
Mn3Cr3(WO8)2 (mp-778921) | 0.7486 | 0.103 | 4 |
LiV(OF)2 (mp-764229) | 0.7372 | 0.026 | 4 |
Mn3V2Cr3O16 (mp-773144) | 0.7443 | 0.084 | 4 |
PtO2 (mp-617) | 0.3626 | 0.005 | 2 |
Rb2O (mp-753746) | 0.2362 | 0.000 | 2 |
PtO2 (mp-7868) | 0.3090 | 0.005 | 2 |
WO2 (mvc-11458) | 0.3048 | 0.206 | 2 |
WO2 (mp-25648) | 0.3349 | 0.206 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sb O |
Final Energy/Atom-5.6677 eV |
Corrected Energy-18.4077 eV
-18.4077 eV = -17.0031 eV (uncorrected energy) - 1.4046 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)