Final Magnetic Moment1.475 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.938 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.204 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.02 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNi3O4 + Al2NiO4 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 337.6 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 281.3 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 160.7 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 297.8 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 198.5 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 297.8 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 99.3 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 281.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 168.8 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 281.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 160.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 136.7 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 56.3 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 198.5 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 297.8 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 99.3 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 281.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 112.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 56.3 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 337.6 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 99.3 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 168.8 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 56.3 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 281.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 337.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 168.8 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 168.8 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 241.0 |
GaSe (mp-1943) | <1 0 0> | <1 0 1> | 198.5 |
BN (mp-984) | <1 1 0> | <0 0 1> | 225.1 |
Al (mp-134) | <1 0 0> | <1 0 1> | 99.3 |
Al (mp-134) | <1 1 0> | <1 0 0> | 160.7 |
Al (mp-134) | <1 1 1> | <0 0 1> | 56.3 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 337.6 |
TeO2 (mp-2125) | <0 0 1> | <1 0 1> | 99.3 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 281.3 |
TeO2 (mp-2125) | <0 1 1> | <1 0 0> | 80.3 |
TeO2 (mp-2125) | <1 0 0> | <0 0 1> | 281.3 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 1> | 297.8 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 337.6 |
C (mp-66) | <1 1 0> | <0 0 1> | 281.3 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 160.7 |
GdScO3 (mp-5690) | <0 1 0> | <0 1 0> | 136.7 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 0> | 136.7 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 56.3 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 1> | 198.5 |
PbS (mp-21276) | <1 0 0> | <1 0 1> | 297.8 |
GaP (mp-2490) | <1 0 0> | <1 0 1> | 297.8 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 0> | 160.7 |
TbScO3 (mp-31119) | <1 0 0> | <0 1 0> | 136.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li10Mn21O48 (mp-698592) | 0.3502 | 0.048 | 3 |
Li6Mn17O40 (mp-763817) | 0.4313 | 0.077 | 3 |
Al4(FeO4)3 (mvc-13141) | 0.4205 | 0.513 | 3 |
Al4(CoO4)3 (mvc-14109) | 0.3909 | 0.288 | 3 |
Li2Mn5O12 (mp-763571) | 0.3863 | 0.310 | 3 |
Zn3Cu10(TeO6)6 (mvc-15145) | 0.7491 | 0.063 | 4 |
TaAl(WO4)2 (mvc-781) | 0.7166 | 0.297 | 4 |
CoO2 (mvc-12170) | 0.5514 | 0.213 | 2 |
FeO2 (mvc-15135) | 0.4953 | 0.278 | 2 |
NiO2 (mvc-13696) | 0.5617 | 0.322 | 2 |
FeO2 (mvc-12125) | 0.5365 | 0.307 | 2 |
FeO2 (mvc-12204) | 0.4867 | 0.269 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Al Ni_pv O |
Final Energy/Atom-5.9789 eV |
Corrected Energy-257.0371 eV
-257.0371 eV = -227.1981 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 12.9840 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)