Final Magnetic Moment0.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.389 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.45 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.227 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI422 [97] |
HallI 4 2 |
Point Group422 |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 281.8 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 148.7 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 169.1 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 56.4 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 56.4 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 267.7 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 169.1 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 89.2 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 267.7 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 281.8 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 148.7 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 159.4 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 267.7 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 327.2 |
TePb (mp-19717) | <1 1 0> | <1 1 1> | 255.2 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 148.7 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 191.2 |
Ag (mp-124) | <1 1 1> | <1 1 0> | 239.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 85.1 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 148.7 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 267.7 |
BN (mp-984) | <1 0 0> | <0 0 1> | 59.5 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 178.5 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 89.2 |
CdTe (mp-406) | <1 1 0> | <1 1 1> | 255.2 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 267.7 |
TeO2 (mp-2125) | <1 0 1> | <1 0 1> | 318.6 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 148.7 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 237.9 |
SiC (mp-7631) | <1 1 1> | <1 0 0> | 169.1 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 0> | 281.8 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 178.5 |
TiO2 (mp-2657) | <1 0 1> | <1 0 1> | 127.5 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 267.7 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <0 0 1> | 119.0 |
C (mp-66) | <1 0 0> | <0 0 1> | 119.0 |
C (mp-66) | <1 1 0> | <0 0 1> | 356.9 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 1> | 63.7 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 89.2 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 267.7 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 1> | 191.2 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 267.7 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 208.2 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 169.1 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 281.8 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 29.7 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 127.5 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 255.2 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 191.2 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 89.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | -0.10272 | 0.10245 | 0.05817 | -0.02394 | -0.04115 |
0.08231 | 0.00000 | -0.08203 | 0.02392 | -0.06888 | 0.05136 |
0.04788 | -0.04785 | 0.00000 | 0.04101 | -0.05122 | 0.01071 |
Piezoelectric Modulus ‖eij‖max0.17927 C/m2 |
Crystallographic Direction vmax |
---|
-2.00000 |
-1.00000 |
-1.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.79 | 0.05 | -0.09 |
0.05 | 2.82 | -0.10 |
-0.09 | -0.10 | 2.93 |
Dielectric Tensor εij (total) |
||
---|---|---|
5.63 | 0.08 | -0.14 |
0.08 | 5.67 | -0.17 |
-0.14 | -0.17 | 5.85 |
Polycrystalline dielectric constant
εpoly∞
2.84
|
Polycrystalline dielectric constant
εpoly
5.72
|
Refractive Index n1.69 |
Potentially ferroelectric?Unknown |
Run TypeGGA |
Energy Cutoff700 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv Cu_pv F |
Final Energy/Atom-4.3495 eV |
Corrected Energy-47.8440 eV
-47.8440 eV = -47.8440 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)