Final Magnetic Moment0.194 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-0.832 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.757 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.05 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFe2O3 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <1 0 0> | <0 0 1> | 301.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 240.9 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 301.2 |
Ag (mp-124) | <1 1 0> | <1 0 -1> | 120.9 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 60.2 |
BN (mp-984) | <1 1 0> | <0 0 1> | 240.9 |
Al (mp-134) | <1 0 0> | <0 0 1> | 240.9 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 232.4 |
SiC (mp-7631) | <1 1 1> | <0 0 1> | 240.9 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 180.7 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 180.7 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 193.2 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 116.2 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 240.9 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 0> | 116.2 |
C (mp-66) | <1 0 0> | <0 0 1> | 301.2 |
C (mp-66) | <1 1 0> | <0 0 1> | 180.7 |
C (mp-66) | <1 1 1> | <0 0 1> | 180.7 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 180.7 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 240.9 |
Au (mp-81) | <1 0 0> | <1 0 1> | 140.2 |
WSe2 (mp-1821) | <1 0 1> | <0 0 1> | 301.2 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 180.7 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 301.2 |
InP (mp-20351) | <1 0 0> | <1 0 1> | 140.2 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 301.2 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 60.2 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 180.7 |
Ga2O3 (mp-886) | <1 1 0> | <0 0 1> | 301.2 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 180.7 |
Au (mp-81) | <1 1 0> | <0 0 1> | 301.2 |
Au (mp-81) | <1 1 1> | <0 0 1> | 60.2 |
WSe2 (mp-1821) | <1 0 0> | <0 0 1> | 301.2 |
ZrO2 (mp-2858) | <0 1 0> | <0 0 1> | 301.2 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 180.7 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 301.2 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 180.7 |
Fe2O3 (mp-24972) | <0 0 1> | <0 0 1> | 180.7 |
Fe2O3 (mp-24972) | <1 0 1> | <0 0 1> | 301.2 |
TiO2 (mp-390) | <0 0 1> | <0 0 1> | 301.2 |
Cu (mp-30) | <1 1 0> | <0 0 1> | 180.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Al4(FeO4)3 (mvc-13141) | 0.4995 | 0.513 | 3 |
Al4(FeO4)3 (mvc-14999) | 0.4868 | 0.164 | 3 |
Al4(FeO4)3 (mvc-15002) | 0.4842 | 0.162 | 3 |
Ti12Fe5O32 (mp-773987) | 0.5033 | 0.108 | 3 |
Ti6Co3O16 (mp-765900) | 0.4958 | 0.236 | 3 |
Zn3Cu10(TeO6)6 (mvc-15145) | 0.7290 | 0.063 | 4 |
KNi3As3O11 (mp-565287) | 0.6749 | 0.000 | 4 |
TaAl(WO4)2 (mvc-781) | 0.6297 | 0.297 | 4 |
MoO2 (mvc-6377) | 0.3194 | 0.299 | 2 |
FeO2 (mvc-12063) | 0.2061 | 0.842 | 2 |
CoO2 (mvc-5466) | 0.1875 | 0.285 | 2 |
MnO2 (mvc-6353) | 0.2794 | 0.246 | 2 |
NiO2 (mvc-6822) | 0.2045 | 0.483 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Fe_pv O |
Final Energy/Atom-5.5752 eV |
Corrected Energy-333.8110 eV
-333.8110 eV = -267.6097 eV (uncorrected energy) - 43.7280 eV (MP Advanced Correction) - 22.4733 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)