Final Magnetic Moment1.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.283 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.090 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.96 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCo2P2O7 + Zn2P2O7 |
Band Gap2.948 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <1 0 0> | <1 1 -1> | 290.6 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 114.3 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 178.4 |
YVO4 (mp-19133) | <1 1 0> | <0 1 1> | 252.2 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 296.9 |
TePb (mp-19717) | <1 1 0> | <1 0 -1> | 306.1 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 178.2 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 296.9 |
BN (mp-984) | <0 0 1> | <0 1 0> | 296.9 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 237.6 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 297.4 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 1> | 228.7 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 252.2 |
AlN (mp-661) | <1 0 1> | <1 0 -1> | 306.1 |
TeO2 (mp-2125) | <0 1 1> | <1 0 1> | 228.7 |
TeO2 (mp-2125) | <1 0 1> | <1 0 1> | 228.7 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 229.5 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 296.9 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 231.0 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 296.9 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 229.5 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 178.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 237.9 |
C (mp-66) | <1 0 0> | <0 1 0> | 178.2 |
C (mp-66) | <1 1 0> | <0 1 0> | 178.2 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 178.2 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 178.2 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 237.6 |
CdTe (mp-406) | <1 0 0> | <0 1 0> | 296.9 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 308.0 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 296.9 |
MgO (mp-1265) | <1 1 1> | <0 1 1> | 252.2 |
TiO2 (mp-2657) | <0 0 1> | <0 1 0> | 296.9 |
TiO2 (mp-2657) | <1 0 1> | <1 0 1> | 228.7 |
TiO2 (mp-2657) | <1 1 1> | <1 1 -1> | 290.6 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 296.9 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 154.0 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 297.4 |
InSb (mp-20012) | <1 1 0> | <1 0 0> | 308.0 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 237.9 |
SiC (mp-11714) | <0 0 1> | <1 0 0> | 231.0 |
SiC (mp-11714) | <1 0 0> | <0 1 1> | 252.2 |
WS2 (mp-224) | <1 1 0> | <0 1 0> | 237.6 |
C (mp-48) | <1 1 1> | <0 0 1> | 237.9 |
ZrO2 (mp-2858) | <0 1 0> | <1 0 -1> | 306.1 |
ZrO2 (mp-2858) | <1 0 -1> | <0 1 1> | 252.2 |
ZrO2 (mp-2858) | <1 1 0> | <0 0 1> | 119.0 |
ZrO2 (mp-2858) | <1 1 1> | <0 1 1> | 252.2 |
CdWO4 (mp-19387) | <0 0 1> | <0 1 1> | 252.2 |
CdWO4 (mp-19387) | <1 0 0> | <0 1 1> | 252.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MgCoP2O7 (mvc-1216) | 0.0762 | 0.108 | 4 |
ZnFeP2O7 (mvc-1240) | 0.0988 | 0.185 | 4 |
ZnCoP2O7 (mvc-13193) | 0.0054 | 0.090 | 4 |
MgNiP2O7 (mvc-1234) | 0.1091 | 0.072 | 4 |
ZnNiP2O7 (mvc-1239) | 0.0746 | 0.070 | 4 |
Ni6P7O24 (mp-504372) | 0.4402 | 0.009 | 3 |
Zn2As2O7 (mp-781624) | 0.4301 | 0.013 | 3 |
Co2P2O7 (mp-25739) | 0.1977 | 0.059 | 3 |
Zn2P2O7 (mp-542331) | 0.2434 | 0.023 | 3 |
Ni2P2O7 (mp-745012) | 0.2451 | 0.000 | 3 |
LiV3Fe2CuO12 (mp-767459) | 0.5334 | 0.209 | 5 |
Li6VNi3(PO4)6 (mp-762748) | 0.6807 | 0.077 | 5 |
Li6CrCo3(PO4)6 (mp-767818) | 0.6906 | 0.064 | 5 |
Li6Mn3Ni(PO4)6 (mp-770421) | 0.6674 | 0.049 | 5 |
Li6VSn3(PO4)6 (mp-775752) | 0.6855 | 0.080 | 5 |
Li4TiCu2Ni3(PO4)6 (mp-776613) | 0.6729 | 0.101 | 6 |
LiMnVP2(O4F)2 (mp-778336) | 0.7409 | 0.002 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Zn Co P O |
Final Energy/Atom-6.5589 eV |
Corrected Energy-315.7527 eV
-315.7527 eV = -288.5926 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction) - 7.4960 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)