Final Magnetic Moment8.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.442 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.308 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.67 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnO + MnS2 + MgO + Y2O3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4m2 [119] |
HallI 4 2 |
Point Group42m |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <1 1 0> | 152.1 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 152.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 337.4 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 220.1 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 29.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 132.0 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 0> | 152.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 161.4 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 190.7 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 205.4 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 264.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 44.0 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 220.1 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 337.4 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 190.7 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 190.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 322.7 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 234.7 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 220.1 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 152.8 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 264.1 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 132.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 73.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 132.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 308.1 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 366.8 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 220.1 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 278.7 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 293.4 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 132.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 249.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 132.0 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 264.1 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 293.4 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 249.4 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 322.7 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 337.4 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 249.4 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 278.7 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 234.7 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 308.1 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 73.4 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 322.7 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 366.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 88.0 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 102.7 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 132.0 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 278.7 |
BN (mp-984) | <0 0 1> | <0 0 1> | 117.4 |
BN (mp-984) | <1 0 0> | <0 0 1> | 58.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Y_sv Mg_pv Mn_pv S O |
Final Energy/Atom-7.2476 eV |
Corrected Energy-95.1709 eV
-95.1709 eV = -86.9708 eV (uncorrected energy) - 4.8384 eV (MP Anion Correction) - 3.3617 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)