Final Magnetic Moment0.284 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.231 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.429 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.15 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBa2CrO4 + BaCr2O4 + Tl2O + BaAl2O4 + Tl |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/mmm [123] |
Hall-P 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 278.5 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 161.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 161.3 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 303.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 190.6 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 263.9 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 190.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 44.0 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 202.2 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 322.5 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 73.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 131.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 249.2 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 263.1 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 263.9 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 285.9 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 293.2 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 234.5 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 73.3 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 263.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 88.0 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 50.5 |
GaSe (mp-1943) | <1 0 0> | <1 0 0> | 202.2 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 278.5 |
BN (mp-984) | <0 0 1> | <0 0 1> | 117.3 |
BN (mp-984) | <1 0 0> | <0 0 1> | 58.6 |
BN (mp-984) | <1 0 1> | <0 0 1> | 249.2 |
BN (mp-984) | <1 1 0> | <1 0 0> | 101.1 |
BN (mp-984) | <1 1 1> | <0 0 1> | 234.5 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 263.9 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 1> | 210.5 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 71.5 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 252.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 202.2 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 219.9 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 29.3 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 205.2 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 131.9 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 44.0 |
MoS2 (mp-1434) | <1 1 0> | <0 0 1> | 117.3 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 202.2 |
GaN (mp-804) | <1 0 0> | <1 1 1> | 218.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 219.9 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 143.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 190.6 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 143.0 |
Al (mp-134) | <1 0 0> | <0 0 1> | 131.9 |
Al (mp-134) | <1 1 0> | <0 0 1> | 249.2 |
Al (mp-134) | <1 1 1> | <1 0 0> | 202.2 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 202.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Ba_sv Al Tl_d Cr_pv O |
Final Energy/Atom-6.4701 eV |
Corrected Energy-93.0537 eV
-93.0537 eV = -84.1117 eV (uncorrected energy) - 4.9160 eV (MP Anion Correction) - 4.0260 eV (MP Advanced Correction)
|