Final Magnetic Moment2.013 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.198 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.098 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.66 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLaCrO3 + CaCrO4 + CaO + La2O3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [148] |
Hall-R 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 208.9 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 238.7 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 139.6 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 208.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 119.4 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 139.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 238.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 171.9 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 208.9 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 238.7 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 139.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 149.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 119.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 29.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 149.2 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 119.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 29.8 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 208.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 119.4 |
BN (mp-984) | <1 0 1> | <0 0 1> | 208.9 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 89.5 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 1> | 142.8 |
Al (mp-134) | <1 0 0> | <0 0 1> | 149.2 |
Al (mp-134) | <1 1 1> | <0 0 1> | 29.8 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 268.6 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 358.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 238.7 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 268.6 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 208.9 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 161.2 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 208.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 238.7 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 89.5 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 328.2 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 208.9 |
LiTaO3 (mp-3666) | <1 0 0> | <1 1 0> | 139.6 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 0> | 241.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 161.2 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 89.5 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 179.0 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 29.8 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 268.6 |
C (mp-66) | <1 0 0> | <0 0 1> | 149.2 |
C (mp-66) | <1 1 0> | <0 0 1> | 149.2 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 358.1 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 238.7 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 1> | 171.9 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 268.6 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 86.0 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 119.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TlNiO3 (mp-998845) | 0.4033 | 0.284 | 3 |
CaTcO3 (mp-998543) | 0.4532 | 0.012 | 3 |
Sr3TeO6 (mp-768907) | 0.3326 | 0.022 | 3 |
Na3AlF6 (mp-676512) | 0.4925 | 0.013 | 3 |
LaAgO3 (mp-768308) | 0.3541 | 0.035 | 3 |
CaLa2FeO6 (mvc-13412) | 0.1415 | 0.090 | 4 |
CaLa2VO6 (mvc-11094) | 0.0837 | 0.041 | 4 |
CaLa2CoO6 (mvc-11031) | 0.1827 | 0.007 | 4 |
CaLa2MnO6 (mvc-11030) | 0.0623 | 0.082 | 4 |
CaLa2TiO6 (mvc-13624) | 0.0805 | 0.063 | 4 |
Pb2O3 (mp-20078) | 0.6162 | 0.009 | 2 |
PtO2 (mp-1285) | 0.5498 | 0.000 | 2 |
CeSe2 (mp-1080328) | 0.5751 | 0.121 | 2 |
CeSe2 (mp-1080851) | 0.5938 | 0.127 | 2 |
YbBr2 (mp-571232) | 0.6054 | 0.001 | 2 |
SrCoBiRuO6 (mp-743579) | 0.7066 | 0.171 | 5 |
SrLaMnMoO6 (mp-690552) | 0.7016 | 0.052 | 5 |
Li4ZrNb(TeO6)2 (mp-756177) | 0.6638 | 0.058 | 5 |
SrLaMnRuO6 (mp-39239) | 0.5628 | 0.084 | 5 |
SrLaMnRuO6 (mp-690590) | 0.6031 | 0.084 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Ca_sv La Cr_pv O |
Final Energy/Atom-7.6961 eV |
Corrected Energy-83.0822 eV
Uncorrected energy = -76.9612 eV
Composition-based energy adjustment (-0.687 eV/atom x 6.0 atoms) = -4.1220 eV
Composition-based energy adjustment (-1.999 eV/atom x 1.0 atoms) = -1.9990 eV
Corrected energy = -83.0822 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)